IP Library Granted Patent US 7,446,139
Granted Patent B2
US 7,446,139 · App. 11/415,516 · Granted Nov 4, 2008

Modified asphalt binder material using crumb rubber and methods of manufacturing a modified asphalt binder

Assignee: Innophos, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,446,139
App. No.
11/415,516
Granted
Nov 4, 2008
Kind
B2
Abstract

In a first aspect, bituminous asphalt binder materials which are modified by the addition of crumb rubber or ground tire rubber are described. In a second aspect, the present invention is directed to methods of producing a modified asphalt binder containing crumb rubber or ground tire rubber. The modified asphalt binders comprise neat asphalt, crumb rubber, one or more synthetic polymers, and one or more acids. The crumb rubber may be obtained from recycled truck and/or automobile tires.

Claims (19)

1. A method for making a modified asphalt binder composition, comprising the steps of:

a. providing neat asphalt in an appropriate vessel;

b. heating the neat asphalt to a temperature of between about 120° C. and about 200° C.;

c. adding to the neat asphalt a first modifying ingredient selected from the group consisting of at least one acid, at least one synthetic polymer and crumb rubber;

d. mixing the asphalt and the first modifying ingredient with one of a high shear mixer or a low shear mixer for a period of between about 5 minutes and about 10 hours

e. adding to the modified asphalt binder a second modifying ingredient selected from the group consisting of at least one acid, at least one synthetic polymer and crumb rubber, wherein the second modifying ingredient is a different type of ingredient than the first modifying ingredient;

f. mixing the second modifying ingredient and the modified asphalt binder in one of a high shear mixer or a low shear mixer for a period of between about 5 minutes and about 10 hours

g. adding to the modified asphalt binder a third modifying ingredient selected from the group consisting of at least one acid, at least one synthetic polymer and crumb rubber, wherein the third modifying ingredient is a different type of ingredient than the first modifying ingredient and the second modifying ingredient; and

h. agitating the third modifying ingredient and the modified binder material in one of a low shear mixer or a high shear mixer for a period of between about 5 minutes and about 48 hours.

2. The method of claim 1 , wherein the step of agitating the third modifying ingredient and the modified binder material is performed in a low shear mixer for a period of between 5 minutes and 10 hours.

3. The method of claim 1 , wherein the first modifying ingredient is between about 0.05% by weight and about 5% by weight of at least one acid, the second modifying ingredient is between about 0.5% by weight and about 30% by weight of at least one synthetic polymer, and the third modifying ingredient is between about 0.5% by weight and about 25% by weight crumb rubber.

4. The method of claim 1 , wherein the first modifying ingredient is between about 0.05% by weight and about 5% by weight of at least one acid, the second modifying ingredient is between about 0.5% by weight and about 25% by weight of crumb rubber, and the third modifying ingredient is between about 0.5% by weight and about 30% by weight of at least one synthetic polymer.

5. The method of claim 1 , wherein the first modifying ingredient is between about 0.5% by weight and about 30% by weight of at least one synthetic polymer, the second modifying ingredient is between about 0.05% by weight and about 5% by weight of at least one acid, and the third modifying ingredient is between about 0.5% by weight and about 25% by weight crumb rubber.

6. The method of claim 5 , wherein the first modifying ingredient is between about 0.5% by weight and about 2% by weight of styrene butadiene styrene, the second modifying ingredient is between about 0.1% by weight and about 1% by weight of polyphosphoric acid, and the third modifying ingredient is between about 4% by weight and about 6% by weight crumb rubber.

7. The method of claim 1 , wherein the first modifying ingredient is between about 0.5% by weight and about 30% by weight of at least one synthetic polymer, the second modifying ingredient is between about 0.5% by weight and about 25% by weight of crumb rubber, and the third modifying ingredient is between about 0.05% by weight and about 5% by weight of at least one acid.

8. The method of claim 7 , wherein the first modifying ingredient is between about 0.5% by weight and about 2% by weight of styrene butadiene styrene, the second modifying ingredient is between about 4% by weight and about 6% by weight of crumb rubber, and the third modifying ingredient is between about 0.1% by weight and about 1% by weight of polyphosphoric acid.

9. The method of claim 1 , wherein the first modifying agent is between about 0.5% by weight and about 25% by weight of crumb rubber, the second modifying agent is between about 0.5% by weight and about 30% by weight of at least one synthetic polymer, and the third modifying agent is between about 0.05% by weight and about 5% by weight of at least one acid.

10. The method of claim 9 , wherein the first modifying agent is between about 4% by weight and about 6% by weight of crumb rubber, the second modifying agent is between about 0.5% by weight and about 2% by weight of styrene butadiene styrene, and the third modifying agent is between about 0.3% by weight and about 1% by weight of polyphosphoric acid.

11. The method of claim 1 , wherein the first modifying agent is between about 0.5% by weight and about 25% by weight of crumb rubber, the second modifying agent is between about 0.05% by weight and about 5% by weight of at least one acid, and the third modifying agent is between about 0.5% by weight and about 30% by weight of at least one synthetic polymer.

Assignments (7)
SECURITY INTEREST Recorded Jan 6, 2025
From: INNOPHOS, INC.
To: WILMINGTON TRUST, NATIONAL ASSOCIATION, AS NOTES COLLATERAL AGENT
Reel/Frame 069749/0169 →
PATENT SECURITY AGREEMENT (ABL) Recorded Feb 10, 2020
From: INNOPHOS, INC.; INNOPHOS, LLC
To: ROYAL BANK OF CANADA, AS COLLATERAL AGENT
Reel/Frame 051858/0131 →
PATENT SECURITY AGREEMENT (TL) Recorded Feb 10, 2020
From: INNOPHOS, INC.; INNOPHOS, LLC
To: ROYAL BANK OF CANADA, AS COLLATERAL AGENT
Reel/Frame 051858/0161 →
RELEASE OF SECURITY INTEREST IN PATENTS Recorded Oct 1, 2010
From: WELLS FARGO BANK, AS SUCCESSOR-BY-MERGER TO WACHOVIA BANK, NATIONAL ASSOCIATION, IN ITS CAPACITY AS AGENT
To: INNOPHOS, INC.
Reel/Frame 025066/0911 →
NOTICE OF GRANT OF SECURITY INTEREST IN PATENTS Recorded Sep 3, 2010
From: INNOPHOS, INC.
To: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS ADMINISTRATIVE AGENT
Reel/Frame 024933/0468 →
SECURITY AGREEMENT Recorded Jun 2, 2009
From: INNOPHOS, INC.
To: WACHOVIA BANK, NATIONAL ASSOCIATION
Reel/Frame 022764/0692 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 2, 2006
From: MARTIN, JEAN-VALERY
To: INNOPHOS, INC.
Reel/Frame 017857/0605 →
Continuity (2)
Provisional Application 6067704000 · May 2, 2005
Related Publication 20060243163A1 · Nov 2, 2006