IP Library Granted Patent US 7,611,596
Granted Patent B2
US 7,611,596 · App. 11/490,372 · Granted Nov 3, 2009

Method of making a dunnage platform

Assignee: Airdex International, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,611,596
App. No.
11/490,372
Granted
Nov 3, 2009
Kind
B2
Abstract

A dunnage platform is in the general shape of a rectangular slab with legs extending form one side. The dunnage platform is made from an expanded polystyrene core. A chemical combination process is used to chemically combine portion of the core proximal to its surface with high impact polystyrene. In a first of two parts of the combination process, the core is placed in a forming mold with one of its two sides and two thirds of its thickness extending therefrom. A heated sheet of high impact polystyrene is brought into contact with the portion of the core extending from the mold. In a similar manner, the other of the two sides of the core is made to extend from the forming mold for contact with a heated sheet of high impact polystyrene.

Claims (14)

1. A process for making a thermoplastic dunnage platform, comprising the steps of:

providing a forming mold adapted to receive an expanded polymer core, wherein said polymer core has been inserted into the forming mold, where a first side of the expanded polymer core and at least half the thickness of the expanded polymer core have been combined with a first high impact polystyrene sheet, wherein the polymer core has been removed from the forming mold;

reinserting the expanded polymer core in the forming mold, wherein a second side of the expanded polymer core and at least half the thickness of the expanded polymer core extend from the mold;

heating a second high impact polystyrene sheet; and

substantially surrounding the second side of the expanded polymer core and at least half the thickness of the expanded polymer core with the second high impact polystyrene sheet.

2. The process of claim 1 , wherein the high impact polystyrene sheet is heated to a temperature in a range of between:

293° F.; and

375° F.

3. The process of claim 1 , further comprising applying reduced pressure to mold the heated high impact polystyrene sheet to the expanded polymer core.

4. The process of claim 1 , wherein the high impact polystyrene sheet is chemically combined with the expanded polymer core.

5. The process of claim 1 , further comprising the steps of:

placing the expanded polymer core in proximity of the high impact polystyrene sheets; and

moving said expanded polymer core into contact with said heated high impact polystyrene sheet.

6. The process of claim 1 , further comprising causing air flow between the heated high impact polystyrene sheet and the expanded polymer core to mold the thermoplastic dunnage platform.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 15, 2016
From: DUMMETT, LAURENCE W
To: AIRDEX INTERNATIONAL, INC.
Reel/Frame 037736/0599 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 15, 2016
From: AIRDEX INTERNATIONAL, INC.
To: AIRDEX CORPORATION
Reel/Frame 037736/0708 →
Continuity (3)
Continuation 1092190300 · Aug 20, 2004
Division 1016698800 · Jun 11, 2002
Related Publication 20060254699A1 · Nov 16, 2006