IP Library Granted Patent US 7,439,294
Granted Patent B2
US 7,439,294 · App. 11/502,814 · Granted Oct 21, 2008

Polyester polymer and copolymer compositions containing metallic titanium particles

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,439,294
App. No.
11/502,814
Granted
Oct 21, 2008
Kind
B2
Abstract

Polyester compositions are disclosed that include polyester polymers or copolymers having incorporated therein metallic titanium particles that improve the reheat properties of the compositions. Processes for making such compositions are also disclosed. The titanium particles may be incorporated in the polyester by melt compounding, or may be added at any stage of the polymerization, such as during the melt-phase of the polymerization. A range of particle sizes may be used, as well as a range of particle size distributions. The polyester compositions are suitable for use in packaging made from processes in which a reheat step is desirable.

Claims (9)

1. A beverage bottle preform having improved reheat, comprising:

a polyester polymer; and

metallic titanium particles, having a median particle size from about 0.005 μm to about 100 μm, dispersed in the polyester polymer.

2. A beverage bottle comprising:

a polyester polymer; and

metallic titanium particles, having a median particle size from about 0.005 μm to about 100 μm, dispersed in the polyester polymer.

3. The beverage bottle preform of claim 1 , wherein the metallic titanium particles are present in an amount of from 5 ppm to 50 ppm, with respect to the total weight of the beverage bottle preform.

4. The beverage bottle preform of claim 1 , wherein the polyester polymer comprises polyethylene terephthalate.

5. The beverage bottle preform of claim 1 , wherein the metallic titanium particles have a median particle size from 0.02 μm to 10 μm, and provide the beverage bottle preform with a reheat improvement temperature (RIT) of at least 5° C. while maintaining preform L* value of 60 or more.

Assignments (2)
CHANGE OF NAME Recorded Jan 11, 2022
From: GRUPO PETROTEMEX, S.A. DE C.V.
To: ALPEK POLYESTER, S.A. DE C.V.
Reel/Frame 058691/0337 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 1, 2011
From: EASTMAN CHEMICAL COMPANY
To: GRUPO PETROTEMEX, S.A. DE C.V.
Reel/Frame 025727/0271 →