Proton exchange membrane (PEM) electrochemical cell having an integral, electrically-conductive, resiliently compressible, porous pad
View Patent ↗Electrolysis cell comprises, in one embodiment, a proton exchange membrane (PEM), an anode positioned along one face of the PEM, and a cathode positioned along the other face of the PEM. A multi-layer metal screen for defining a first fluid cavity is placed in contact with the outer face of the anode, and an electrically-conductive, compressible, spring-like, porous pad for defining a second fluid cavity is placed in contact with the outer face of the cathode. The porous pad comprises a mat of carbon fibers bound together with one or more, preferably thermoplastic, resins, the mat having a density of about 0.2-1.5 g/cm 3 . Cell frames are placed in peripheral contact with the metal screen and the compression pad for peripherally containing fluids present therewithin. Electrically-conductive separators are placed in contact with the metal screen and the compression pad for axially containing fluids present therewithin. A plurality of the cells may be arranged in series in a bipolar configuration without requiring a separate compression pad between cells (for gas pressure differentials up to about 400 psi or greater). The invention is also directed to a fuel cell wherein the pad replaces the carbon fiber paper or carbon fiber cloth in contact with the cathode or anode.
1. An electrochemical cell stack comprising two electrochemical cells arranged in series in a bipolar configuration and electrically coupled to one another, each one of said two electrochemical cells comprising a proton exchange membrane having a first face and a second face, an anode positioned along said first face of said proton exchange membrane, a cathode positioned along said second face of said proton exchange membrane, and a compression pad for use in defining a cathodic fluid cavity, said compression pad being electrically-conductive, resiliently compressible and porous and having an inner face and an outer face.
2. The electrochemical cell stack as claimed in claim 1 wherein each of said electrochemical cells is a fuel cell.
3. The electrochemical cell stack as claimed in claim 1 wherein said compression pad comprises a random mat of carbon fibers bound together using one or more binders including at least one thermoplastic binder.
4. The electrochemical cell stack as claimed in claim 3 wherein said at least one thermoplastic binder comprises a polyvinylidene fluoride (PVDF).
5. The electrochemical cell stack as claimed in claim 3 wherein said at least one thermoplastic binder comprises a combination of a PVDF and polytetrafluoroethene (PTFE).
6. The electrochemical cell stack as claimed in claim 3 wherein said compression pad further comprises a waterproofing coating applied to at least one side of said random mat, said waterproofing coating comprising PTFE and electron-conducting carbon particles.
7. The electrochemical cell stack as claimed in claim 3 wherein said compression pad further comprises a waterproofing coating applied to at least one side of said random mat, said waterproofing coating comprising electron-conducting carbon particles functionalized with hydrophobic organic groups.
8. The electrochemical cell stack as claimed in claim 1 wherein said compression pad comprises a stack of carbon fiber papers, each of said carbon fiber papers comprising a plurality of carbon fibers bound together with a first thermosetting binder, each of said carbon fiber papers being bound to an adjacent carbon fiber paper in said stack with a second thermosetting binder.
9. The electrochemical cell stack as claimed in claim 1 wherein said compression pad has a density of about 0.2-1.5 g/cm 3 .
10. The electrochemical cell stack as claimed in claim 9 wherein said compression pad has a density of about 0.35-0.77 g/cm 3 .
11. The electrochemical cell stack as claimed in claim 10 wherein said compression pad has a density of about 0.55-0.77 g/cm 3 .
12. The electrochemical cell stack as claimed in claim 1 wherein said compression pad, after being compressed to pressures up to about 12,000 psi, has an uncompressed thickness of at least 70% of its original, pre-compressed thickness.