Mixture for anode of improved adhesive strength and lithium secondary battery containing the same
View Patent ↗Provided is an anode mix for a secondary battery comprising an anode active material, a conductive material and a binder, wherein the anode mix contains 0.01 to 1.0% by weight of alumina having an average particle diameter of less than 1000 nm, based on the total weight of the mix, and a lithium secondary battery comprising the same. Therefore, the present invention can achieve increases in anode active material-conductive material adhesion and anode active material-current collector adhesion which are exerted by a binder, and ultimately can improve lifespan characteristics or cycle characteristics of the battery.
1. A lithium secondary battery, comprising:
an electrode assembly composed of a cathode and an anode, which are disposed opposite with respect to each other and have a separator therebetween, and a non-aqueous electrolyte containing a lithium salt,
wherein an anode mix for the anode comprises an anode active material, a conductive material, a binder and 0.05 to 0.5% by weight of alumina having an average particle diameter of 10 to 400 nm, based on the total weight of the mix; and
a cathode active material for the cathode is a lithium transition metal oxide; and
the lithium salt is selected from the group consisting of LiCl, LiBr, LiI, LiClO 4 , LiBF 4 , LiB 10 Cl 10 , LiPF 6 , LiCF 3 SO 3 , LiCF 3 CO 2 , LiAsF 6 , LiSbF 6 , LiAlCl 4 , CH 3 SO 3 Li, CF 3 SO 3 Li, LiSCN, LiC(CF 3 SO 2 ) 3 , (CF 3 SO 2 ) 2 NLi, a lithium chloroborate, a lithium lower aliphatic carboxylate, lithium tetraphenyl borate, and a lithium imide.