IP Library Granted Patent US 7,297,831
Granted Patent B2
US 7,297,831 · App. 11/557,574 · Granted Nov 20, 2007

Process of preparing aromatic hydrocarbons and liquefied petroleum gas from hydrocarbon mixture

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,297,831
App. No.
11/557,574
Granted
Nov 20, 2007
Kind
B2
Abstract

Disclosed is a process of preparing aromatic hydrocarbons and liquefied petroleum gas (LPG) from a hydrocarbon mixture, in which a non-aromatic compound in the hydrocarbon feedstock mixture is converted into a gaseous material having a large amount of LPG through hydrocracking, and an aromatic compound therein is converted into an oil component having large amounts of benzene, toluene, and xylene (BTX) through dealkylation and transalkylation, in the presence of a catalyst obtained by supporting platinum/bismuth onto a mixture support having zeolite and an inorganic binder. The gaseous product is separated into LPG and a mixture of methane and ethane depending on differences in boiling point through distillation, while the liquid product is separated into benzene, toluene, xylene, and C9+ aromatic compounds depending on differences in boiling point through distillation.

Claims (33)

1. A method of preparing aromatic hydrocarbons and liquefied petroleum gas (LPG) from a hydrocarbon mixture, comprising the following steps of:

(a) introducing a hydrocarbon feedstock mixture and hydrogen into at least one reaction zone;

(b) converting the hydrocarbon feedstock mixture in the presence of a catalyst to (i) a non-aromatic hydrocarbon compound which is abundant in LPG through hydrocracking and to (ii) an aromatic hydrocarbon compound which is abundant in benzene, toluene and xylene (BTX) through dealkylation/transalkylation within the reaction zone; and

(c) recovering the LPG and aromatic hydrocarbon compound, respectively from the reaction products of step (b) through gas-liquid separation and distillation,

wherein the catalyst is prepared by supporting 0.01˜0.5 parts by weight of platinum (Pt) and 0.01˜3.0 parts by weight of bismuth (Bi) onto 100 parts by weight of a mixture support, the mixture support including 10˜95 wt % of zeolite having a molar ratio of silica/alumina of 200 or less, selected from the group consisting of mordenite, β-zeolite, ZSM-5 zeolite and combinations thereof, and 5˜90 wt % of an inorganic binder.

2. The method according to claim 1 , further comprising separating the aromatic hydrocarbon compound recovered in step (c) into benzene, toluene, xylene and C9+ aromatic compounds, respectively.

3. The method according to claim 1 , wherein a molar ratio of hydrogen and hydrocarbon feedstock mixture in step (a) is 0.5˜10, and the hydrocarbon feedstock mixture, which is introduced into the reaction zone, has a space velocity of 0.5˜10 hr −1 .

4. The method according to claim 1 , wherein step (b) is conducted at 250˜600° C. under a pressure of 5˜50 atm.

5. The method according to claim 1 , wherein the hydrocarbon feedstock mixture is selected from the group consisting of reformate, pyrolysis gasoline, C9+ aromatic compound-containing mixtures, naphtha, and combinations thereof.

6. The method according to claim 1 , wherein the mixture support has an average pore diameter of 50˜200 Å, a pore volume of 0.1˜1 cc, a specific surface area of 200˜400 m 2 /g and an apparent bulk density of 0.4˜1.0 cc/g.

7. The method according to claim 1 , wherein the inorganic binder is selected from the group consisting of bentonite, kaoline, clinoptilolite, montmorillonite, γ-alumina, silica, silica-alumina, and combinations thereof.

8. The method according to claim 1 , wherein the catalyst is prepared by mixing zeolite, the inorganic binder, platinum and bismuth; and molding the mixture.

9. The method according to claim 1 , wherein the catalyst is prepared by mixing zeolite and the inorganic binder, followed by molding the mixture; supporting bismuth onto the molded mixture support; and supporting platinum onto the bismuth-supported mixture support.

10. The method according to claim 1 , wherein the catalyst is prepared by mixing zeolite and the inorganic binder; supporting an admixture comprising platinum and bismuth onto the mixture support; and molding the supported mixture support.

11. The method according to claim 1 , wherein the catalyst is prepared by supporting platinum onto zeolite; mixing the platinum-supported zeolite and the inorganic binder, followed by molding the mixture; and supporting bismuth onto the platinum-supported mixture support.

12. The method according to claim 1 , wherein the catalyst is prepared by mixing zeolite and the inorganic binder, followed by molding the mixture support, while supporting either platinum or bismuth onto the mixture support; and supporting the other metal, which is not supported in a previous step, onto the mixture support.

13. A method of preparing aromatic hydrocarbons and LPG from a hydrocarbon mixture, comprising the following steps of:

(a) introducing a hydrocarbon feedstock mixture and hydrogen into at least one reaction zone;

(b) converting the hydrocarbon feedstock mixture in the presence of a catalyst to (i) a non-aromatic hydrocarbon compound which is abundant in LPG through hydrocracking and to (ii) an aromatic hydrocarbon compound which is abundant in BTX through dealkylation/transalkylation within the reaction zone;

(c) separating the reaction products of step (b) into an overhead stream including hydrogen, methane, ethane and LPG and a bottom stream including the aromatic hydrocarbon compound, and residual hydrogen and non-aromatic hydrocarbon compound, through gas-liquid separation;

(d) recovering the LPG from the overhead stream; and

(e) recovering the aromatic hydrocarbon compound from the bottom stream,

wherein the catalyst is prepared by supporting 0.01˜0.5 parts by weight of platinum (Pt) and 0.01˜3.0 parts by weight of bismuth (Bi) onto 100 parts by weight of a mixture support, the mixture support comprising 10˜95 wt % of zeolite having a molar ratio of silica/alumina of 200 or less, selected from the group consisting of mordenite, β-zeolite, ZSM-5 zeolite and combinations thereof, and 5˜90 wt % of an inorganic binder.

14. The method according to claim 13 , further comprising separating the aromatic hydrocarbon compound recovered in step (e) into benzene, toluene, xylene and C9+ aromatic compounds, respectively.

15. A method of preparing aromatic hydrocarbons and LPG from a hydrocarbon mixture, comprising the following steps of:

(a) introducing the hydrocarbon feedstock mixture and hydrogen into at least one reaction zone;

(b) converting the hydrocarbon feedstock mixture in the presence of a catalyst to (i) a non-aromatic hydrocarbon compound which is abundant in LPG through hydrocracking and to (ii) an aromatic hydrocarbon compound which is abundant in BTX through dealkylation/transalkylation within the reaction zone;

(c) separating the reaction products of step (b) into a first overhead stream including hydrogen, methane, ethane and LPG and a first bottom stream including the aromatic hydrocarbon compound, and residual hydrogen and non-aromatic hydrocarbon compound, through gas-liquid separation;

(d) recovering the LPG from the first overhead stream; and

(e) separating the first bottom stream into (i) a second overhead stream including the residual hydrogen and the non-aromatic hydrocarbon compound and (ii) a second bottom stream including the aromatic hydrocarbon compound, through distillation; and

(f) recovering the LPG from the second overhead stream and recovering the aromatic hydrocarbon compound from the second bottom stream,

wherein the catalyst is prepared by supporting 0.01˜0.5 parts by weight of platinum (Pt) and 0.01˜3.0 parts by weight of bismuth (Bi) onto 100 parts by weight of a mixture support, the mixture support comprising 10˜95 wt % of zeolite having a molar ratio of silica/alumina of 200 or less, selected from the group consisting of mordenite, β-zeolite, ZSM-5 zeolite and combinations thereof, and 5˜90 wt % of an inorganic binder.

16. The method according to claim 15 , further comprising separating the aromatic hydrocarbon compound recovered in step (f) into benzene, toluene, xylene and C9+ aromatic compounds, respectively.

Assignments (4)
CORRECTIVE ASSIGNMENT TO CORRECT THE INCORRECT PATENT NUMBER 7448700 AND REPLACE IT WITH 7488700 PREVIOUSLY RECORDED ON REEL 026619 FRAME 0330. ASSIGNOR(S) HEREBY CONFIRMS THE CHANGE OF NAME. Recorded Apr 11, 2016
From: SK ENERGY CO., LTD.
To: SK INNOVATION CO., LTD.
Reel/Frame 038406/0201 →
CHANGE OF NAME Recorded Jul 14, 2011
From: SK ENERGY CO., LTD.
To: SK INNOVATION CO., LTD.
Reel/Frame 026619/0330 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 14, 2007
From: SK CORPORATION
To: SK ENERGY CO., LTD
Reel/Frame 020249/0017 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 21, 2006
From: LEE, JONG HYUNG; OH, SEUNG HOON; SUNG, KYOUNG HAK; CHOI, SUN; KIM, YONG SEUNG; LIM, BYEUNG SOO
To: SK CORPORATION
Reel/Frame 018541/0036 →