US 8,087,966 · App. 11/568,037 · Granted Jan 3, 2012

Method for the thermal treatment of tungsten electrodes free from thorium oxide for high-pressure discharge lamps

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,087,966
App. No.
11/568,037
Granted
Jan 3, 2012
Kind
B2
Abstract

The invention relates to a method for the thermal treatment of tungsten electrodes having a fibrous mocrostructure and being free from thorium oxide for high-pressure discharge lamps, to such a tungsten electrode free from thorium oxide, to a method of manufacturing a high-pressure gas discharge lamp with at least one such tungsten electrode free from thorium oxide, to a high-pressure gas discharge lamp with at least one such tungsten electrode free from thorium oxide, and to a lighting unit with at least one such high-pressure gas discharge lamp.

Claims (13)

1. A method for the thermal treatment of tungsten electrodes free from thorium oxide for high-pressure discharge lamps, characterized in that the tungsten electrodes consist of pure tungsten or of tungsten doped with at least potassium, wherein said electrodes have a fibrous microstructure, and the maximum temperature during the thermal treatment is lower than the recrystallization temperature of the material of the tungsten electrodes;

wherein the thermal treatment yields a cleaning of the electrode surface.

2. A method as claimed in claim 1 , characterized in that the method, which is carried out in an oxygen-free atmosphere at normal atmospheric pressure, comprises at least the following sequence of steps: heating up from room temperature to the maximum processing temperature, keeping at the maximum processing temperature, and cooling down to room temperature.

3. A method as claimed in claim 2 , characterized in that the method is carried out in an atmosphere that contains hydrogen.

4. A method as claimed in claim 1 , characterized in that the tungsten electrodes consist of tungsten doped with at most 500 ppm of potassium, at most 300 ppm of silicon, and at most 100 ppm of aluminum.

5. A method as claimed in claim 1 , characterized in that the recrystallization temperature of the material of the tungsten electrodes is approximately 1600° C. to 1800° C., and maximum processing temperature is approximately 1500° C.

6. A tungsten electrode free from thorium oxide and treated by a method as claimed in claim 1 .

7. A method of manufacturing a high-pressure gas discharge lamp with at least one tungsten electrode free from thorium oxide, comprising at least a method for the thermal treatment of tungsten electrodes free from thorium oxide as claimed in claim 1 .

8. A high-pressure gas discharge lamp with at least one tungsten electrode free from thorium oxide designed for automobile headlights and manufactured by a method as claimed in claim 7 .

9. A high-pressure gas discharge lamp according to claim 1 , wherein a portion of the tungsten electrode free from thorium oxide is enclosed by a seal or pinch, characterized in that the portion of the tungsten electrode free from thorium oxide enclosed by the seal or pinch has a fibrous microstructure.

10. A lighting unit comprising at least one high-pressure discharge lamp as claimed in claim 9 .

11. A method for the thermal treatment of tungsten electrodes free from thorium oxide for high-pressure discharge lamps, characterized in that the tungsten electrodes consist of pure tungsten or of tungsten doped with at least potassium, wherein said electrodes have a fibrous microstructure, and the maximum temperature during the thermal treatment is lower than the recrystallization temperature of the material of the tungsten electrodes; and,

wherein the fibrous microstructure remains intact until first operation.

Assignments (7)
RELEASE OF SECURITY INTEREST Recorded Jan 29, 2025
From: SOUND POINT AGENCY LLC
To: LUMILEDS LLC; LUMILEDS HOLDING B.V.
Reel/Frame 070046/0001 →
SECURITY INTEREST Recorded Jan 5, 2023
From: LUMILEDS LLC; LUMILEDS HOLDING B.V.
To: SOUND POINT AGENCY LLC
Reel/Frame 062299/0338 →
CHANGE OF NAME Recorded Oct 31, 2018
From: KONINKLIJKE PHILIPS ELECTRONICS N.V.
To: KONINKLIJKE PHILIPS N.V.
Reel/Frame 047368/0237 →
CORRECTIVE ASSIGNMENT TO CORRECT THE CONVEYING PARTY DATA PREVIOUSLY RECORDED AT REEL: 044931 FRAME: 0651. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded Aug 13, 2018
From: KONINKLIJKE PHILIPS N.V.
To: LUMILEDS LLC
Reel/Frame 047304/0203 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 21, 2017
From: KONINKLIJKE PHILIPS ELECTRONICS N.V.
To: LUMILEDS LLC
Reel/Frame 044931/0651 →
SECURITY INTEREST Recorded Jul 7, 2017
From: LUMILEDS LLC
To: DEUTSCHE BANK AG NEW YORK BRANCH, AS COLLATERAL AGENT
Reel/Frame 043108/0001 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 18, 2006
From: HEBBINGHAUS, GERHARD; MERX, JOZEF
To: KONINKLIJKE PHILIPS ELECTRONICS N V
Reel/Frame 018405/0159 →