IP Library Granted Patent US 7,942,998
Granted Patent B2
US 7,942,998 · App. 11/582,351 · Granted May 17, 2011

Method and apparatus for laser welding thermoplastic resin members

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,942,998
App. No.
11/582,351
Granted
May 17, 2011
Kind
B2
Abstract

A method and apparatus for welding members formed of thermoplastic resin material, with high welding strength and small strength variations. A laser welding apparatus 1 brings a first member 2 formed of a transmissive thermoplastic resin that transmits a laser beam into contact with a second member 3 formed of an absorptive thermoplastic resin that absorbs the laser beam, and joins the thermoplastic resin members by melting their contact surfaces 4 with the laser beam. The laser welding apparatus 1 further comprises a laser beam generator 10 for irradiating the contact surfaces with the laser beam shone from the side of the first member 3 so as to melt at least one of the contact surfaces of the first member and the second member. The apparatus also comprises a clamp mechanism 20 for pressing the first member and the second member together, a temperature sensor 31 as an adjusting means for adjusting the pressing force applied to the first member and the second member, and a personal computer 32 for calculating the pressing force based on the output of the temperature sensor. The clamp mechanism is controlled with the calculated pressing force.

Claims (6)

1. A method for laser welding thermoplastic resin members which comprises bringing a first member formed of a transmissive thermoplastic resin that transmits a laser beam into contact with a second member formed of an absorptive thermoplastic resin that absorbs the laser beam, and melting their contact surfaces with the laser beam for joining the members, said method further comprising:

pressing the first member and the second member together by a pressing force;

irradiating the contact surfaces of the two members with a laser beam shone from the side of the first member; melting at least one of the contact surfaces of the two members; and

welding the two members while adjusting the pressing force applied to the first member and the second member;

wherein the adjustment of the pressing force is directly controlled based on a detected temperature at a melted portion of the contact surfaces that is melted by laser beam irradiation, and

wherein in the adjustment of the pressing force, the pressing force is increased to a first pressing force when a detected temperature is greater than a predetermined value, and the pressing force is further increased to a second pressing force when another detected temperature indicates cooling at the melted portion.

Assignments (3)
CHANGE OF NAME Recorded Feb 11, 2026
From: DUPONT POLYMERS, INC.
To: CELANESE POLYMERS HOLDING, INC.
Reel/Frame 074734/0498 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 26, 2019
From: E. I. DU PONT DE NEMOURS AND COMPANY
To: DUPONT POLYMERS, INC.
Reel/Frame 049590/0650 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 18, 2006
From: WATANABE, TOSHIO; NAKAJIMA, KATSUHIKO; NAKAMURA, HIDEO; MORI, HIROSHI; FUJITA, SUSUMU; NAKATANI, MITSUNOBU
To: TOYOTA JIDOSHA KABUSHIKI KAISHA; E.I. DU PONT DE NEMOURS AND COMPANY
Reel/Frame 018426/0906 →