Method for blending heat-sensitive material using a conical screw blender with gas injection
View Patent ↗The invention relates to a conical screw blender which comprises an inverted cone-shaped vessel. The blender also includes a material inlet, a material outlet, a driven screw housed within the vessel, and at least two non-diffuse gas injection lines attached to the vessel. The conical screw blender of the present invention can be used not only for the mixing of materials, but also for the drying of materials.
1. A method for drying heat-sensitive materials comprising:
a.) introducing at least one heat-sensitive material and at least one other material into a conical screw blender wherein said blender comprises:
i. an inverted cone-shaped vessel;
ii. a material inlet in the vessel;
iii. a material outlet located at or near the bottom of the vessel;
iv. a driven screw housed within the vessel; and
v. at least two non-diffused gas injection lines attached to the vessel and adapted to inject an inert purging agent into the vessel, wherein at least one gas injection line is located near the base of the vessel, and said gas injection lines act to reduce shearing stress of the driven screw on a material introduced through said material inlet and to displace atmospheric oxygen from within said vessel;
b.) blending the at least one heat-sensitive material and other material; and
c.) introducing at least two streams of an inert purging agent into the blender at a rate which causes the materials to form a local spouting bed motion, wherein the purging
agent is selected from the group consisting of nitrogen gas and carbon dioxide gas.
2. The method according to claim 1 wherein the purging agent is introduced at a rate of between about 3 and 7 SCFM.
3. The method according to claim 1 , wherein the purging agent is introduced at a rate of about 5 SCFM.
4. The method according to claim 1 , wherein the purging agent is introduced at a temperature below about 25° C.
5. The method according to claim 1 , wherein the purging agent is introduced at a temperature of about 10° C.
6. The method according to claim 1 wherein the purging agent is introduced at a temperature of about 0° C.