Compositions of corrosion-resistant Fe-based amorphous metals suitable for producing thermal spray coatings

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,480,864
App. No.
11/595,166
Granted
Jul 9, 2013
Kind
B2
Abstract

A method of coating a surface comprising providing a source of amorphous metal that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses: chromium (15 to 20 atomic %), molybdenum (2 to 15 atomic %), tungsten (1 to 3 atomic %), boron (5 to 16 atomic %), carbon (3 to 16 atomic %), and the balance iron; and applying said amorphous metal to the surface by a spray.

Claims (52)

1. An apparatus, comprising:

a deposition chamber,

an amorphous metal deposition system in said deposition chamber that produces two amorphous metal deposition sprays, a first amorphous metal deposition spray and a second amorphous metal deposition spray,

said first amorphous metal deposition spray and said second amorphous metal deposition spray in said deposition chamber being corrosion-resistant amorphous metal deposition material that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses:

chromium (15 to 20 atomic %),

molybdenum (2 to 15 atomic %),

tungsten (1 to 3 atomic %),

boron (5 to 16 atomic %),

carbon (3 to 16 atomic %), and

the balance iron;

said first amorphous metal deposition spray and said second amorphous metal deposition spray producing a composite amorphous metal material made of corrosion-resistant amorphous metal that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses:

chromium (15 to 20 atomic %),

molybdenum (2 to 15 atomic %),

tungsten (1 to 3 atomic %),

boron (5 to 16 atomic %),

carbon (3 to 16 atomic %), and

the balance iron; and

wherein said amorphous metal deposition system in said deposition chamber directs said first amorphous metal deposition spray and said second amorphous metal deposition spray onto metal armor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant, said amorphous metal deposition system directing a

first layer and a second layer of corrosion-resistant amorphous-metal coating on said metal armor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant, wherein said corrosion-resistant amorphous-metal coating is made of amorphous metal that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses:

chromium (15 to 20 atomic %),

molybdenum (2 to 15 atomic %),

tungsten (1 to 3 atomic %),

boron (5 to 16 atomic %),

carbon (3 to 16 atomic %), and

the balance iron,

wherein said first amorphous metal deposition spray and said second amorphous metal deposition spray have different compositions and wherein said first layer and said second layer having different compositions direct a graded corrosion-resistant amorphous-metal coating on said metal armor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant.

2. An apparatus for producing a corrosion resistant amorphous metal coating on a structure to be coated including metal armor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant, comprising:

a deposition chamber with the structure to be coated in said deposition chamber,

an amorphous metal deposition system in said deposition chamber that produces two amorphous metal deposition sprays, a first amorphous metal deposition spray and a second amorphous metal deposition spray, said amorphous metal deposition system including a magnetron and a sputter target,

said first amorphous metal deposition spray and said second amorphous metal deposition spray being made of a amorphous metal deposition material that is corrosion-resistant amorphous metal deposition material that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses:

chromium (15 to 20 atomic %),

molybdenum (2 to 15 atomic %),

tungsten (1 to 3 atomic %),

boron (5 to 16 atomic %),

carbon (3 to 16 atomic %), and

the balance iron;

said first amorphous metal deposition spray and said second amorphous metal deposition spray producing a composite amorphous metal material made of corrosion-resistant amorphous metal that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses:

chromium (15 to 20 atomic %),

molybdenum (2 to 15 atomic %),

tungsten (1 to 3 atomic %),

boron (5 to 16 atomic %),

carbon (3 to 16 atomic %), and

the balance iron; and

wherein said amorphous metal deposition system in said deposition chamber directs said first amorphous metal deposition spray and said second amorphous metal deposition spray onto the structure to be coated including metal minor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant, said amorphous metal deposition system directing a

first layer and a second layer of corrosion-resistant amorphous-metal coating on the structure to be coated including metal armor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant, wherein said corrosion-resistant amorphous-metal coating is made of amorphous metal that contains manganese (1 to 3 atomic %), yttrium (0.1 to 10 atomic %), and silicon (0.3 to 3.1 atomic %) in the range of composition given in parentheses; and that contains the following elements in the specified range of composition given in parentheses:

chromium (15 to 20 atomic %),

molybdenum (2 to 15 atomic %),

tungsten (1 to 3 atomic %),

boron (5 to 16 atomic %),

carbon (3 to 16 atomic %), and

the balance iron,

wherein said first amorphous metal deposition spray and said second amorphous metal deposition spray have different compositions and wherein said first layer and said second layer having different compositions direct a graded corrosion-resistant amorphous-metal coating on the structure to be coated including metal armor or projectiles or gun barrels or tank loader trays or rail guns or non-magnetic hulls or hatches or seals or propellers or rudders or pump impellers and shafts or containers for spent nuclear fuel or pressurized water reactors or boiling water reactors or breeder reactors with liquid metal coolant.

Assignments (3)
50% UNDIVIDED INTEREST Recorded Oct 4, 2007
From: REGENTS OF THE UNIVERSITY OF CALIFORNIA, THE
To: LAWRENCE LIVERMORE NATIONAL SECURITY, LLC
Reel/Frame 020012/0178 →
CONFIRMATORY LICENSE Recorded Apr 11, 2007
From: CALIFORNIA, THE REGENTS OF THE UNIVERSITY OF
To: ENERGY, U.S. DEPARTMENT OF
Reel/Frame 019155/0885 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 21, 2006
From: FARMER, JOSEPH C.; WONG, FRANK M.G.; HASLAM, JEFFERY J.; DAY, SUMNER D.; LAVERNIA, ENRIQUE J.