US 7,287,907 · App. 11/668,398 · Granted Oct 30, 2007

Surface densification of powder metal bearing caps

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,287,907
App. No.
11/668,398
Granted
Oct 30, 2007
Kind
B2
Abstract

A high performance main bearing cap has particular surfaces densified for improved fatigue crack resistance. The surfaces densified are the bolted face inside of a perimetral margin and outside of bolt head interface areas around the main bolt holes, the surfaces of the main bolt holes and the side bolt hole threads. Preferred methods of densification are single needle programmable pattern peening of the bolted face peened area, over-burnishing of the bolt holes, and forming the threads rather than cutting them for the side bolt threads.

Claims (9)

1. In a powder metal bearing cap which has a bore arch in a bridging section between two legs of said bearing cap, with bolt holes extending through the legs from a bolted face of said bearing cap which is opposite from said bore arch to a joint face of each leg, said joint face being opposite from said bolted face with one joint face on each side of said arch, said bearing cap further including side bolt holes in end surfaces of the bearing cap the improvement wherein at least one of said bolt holes and said side bolt holes are surface densified.

2. The improvement of claim 1 , wherein said bolt holes are surface densified by compressing the surfaces of the holes so as to expand the diameter of each hole by at least 0.10 mm.

3. The improvement of claim 1 , wherein said bolt holes are surface densified at least adjacent to the joint face.

4. The improvement of claim 1 , wherein said bolt holes are surface densified over substantially their whole length.

5. The improvement of claim 1 , wherein said bolt holes are surface densified by compressing the surfaces of the holes so as to expand the diameter of each hole.

6. the improvement of claim 1 , wherein said side bolt holes have formed threads.

7. The improvement of claim 6 , wherein said threads in said side bolt holes are formed by roll forming.

8. The improvement of claim 6 , wherein said threads in said side bolt holes are densified to a depth that resists stripping of the threads.

9. The improvement of claim 6 , wherein said threads in said side bolt holes are formed by deformation.