1 . A method of manufacturing nonfibrous casing, wherein the casing is made from a viscose solution that is extruded as a tube into a coagulation and regenerating bath, thereby producing a cellulosic tube in a gel state, which gel tube is ultimately dried, the improvement comprising applying to the interior of the dried casing a liquid smoke composition having a dilutable tar content of from greater than about 1.0 wt % to about 9.0 wt %, a pH greater than about 4.5, a Karl Fischer percent moisture of from about 20 to about 34 wt %, a staining index of greater than about 140, at least one anionic surfactant, and optionally, a wax.
2 . A method of manufacturing nonfibrous casing according to claim 1 , wherein the dilutable tar content ranges from about 2.9 to about 5 wt. %.
3 . A method of manufacturing nonfibrous casing according to claim 1 , wherein the pH is from about 5.0 to about 5.4.
4 . A method of manufacturing nonfibrous casing according to claim 1 , wherein the casing is multilayer and contains an inner layer of nylon or plastic.
5 . A method of manufacturing nonfibrous casing according to claim 1 , wherein the casing is multilayer and contains an outer layer of nylon or plastic.
6 . A method of manufacturing according to claim 1 , wherein the surfactant is sodium lauryl sulfate.
7 . A method of manufacturing according to claim 1 , wherein the surfactant is dodecyl benzene sulfonate.
8 . A method of manufacturing according to claim 1 , wherein the surfactant is sodium lauryl sulfate and dodecyl benzene sulfonate.
9 . A casing comprising a nonfibrous cellulosic casing containing on its interior surface a liquid smoke composition having a dilutable tar content of greater than about 1.0 wt % to about 9.0 wt %, a pH greater than about 4.5, a Karl Fischer percent moisture of from about 20 to about 34 wt %, a staining index of greater than about 140, at least one anionic surfactant, and optionally, a wax.
10 . A casing according to claim 9 , wherein the dilutable tar content ranges from about 2.9 to about 5 wt. %.
11 . A casing according to claim 9 , wherein the pH is from about 5.0 to about 5.4.
12 . A casing according to claim 9 , wherein the surfactant is sodium lauryl sulfate.
13 . A casing according to claim 9 , wherein the surfactant is dodecyl benzene sulfonate.
14 . A casing according to claim 9 , wherein the surfactant is sodium lauryl sulfate and dodecyl benzene sulfonate.
15 . A casing according to claim 9 , wherein the casing is multilayer and contains an inner layer of nylon or plastic.
16 . A casing according to claim 9 , wherein the casing is multilayer and contains an outer layer of nylon or plastic.
17 . A casing comprising a nonfibrous nylon or plastic casing containing on its interior surface a liquid smoke composition having a dilutable tar content of greater than about 1.0 wt % to about 9.0 wt %, a pH greater than about 4.5, a Karl Fischer per cent moisture of from about 20 to about 34 wt %, a staining index of greater than about 140, at least one anionic surfactant, and optionally, a wax.