IP Library Granted Patent US 8,010,022
Granted Patent B2
US 8,010,022 · App. 11/730,647 · Granted Aug 30, 2011

Developing roller and method of producing the same, and inspection process for developing roller product

Assignee: Bridgestone Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,010,022
App. No.
11/730,647
Granted
Aug 30, 2011
Kind
B2
Abstract

A developing roller having a properly adjusted toner feed quantity comprises a shaft, an elastic layer and a surface covering layer, in which a JIS 10-point average roughness (Rz) of the surface is 4-7 μm and a specular gloss at 85° according to JIS Z8741 of the surface is 14-55.

Claims (7)

1. A developing roller comprising a shaft, an elastic layer formed on an outer periphery of the shaft, and a surface covering layer formed on an outer peripheral face of the elastic layer, wherein a JIS 10-point average roughness (Rz) of the surface is 4-7 μm and a specular gloss at 85° according to JIS Z8741 of the surface is 14-55, and wherein the surface covering layer is formed by preparing a paint inclusive of a component constituting the surface covering layer, leaving at room temperature and normal humidity for not less than 24 hours and then applying the paint onto the outer peripheral face of the elastic layer.

2. A developing roller according to claim 1 , wherein the elastic layer is made from polyurethane.

3. A developing roller according to claim 1 , wherein the surface covering layer is made from a crosslinking resin.

4. A developing roller according to claim 3 , wherein the crosslinking resin is a polyurethane resin.

5. A developing roller according to claim 1 , wherein the JIS 10-point average roughness (Rz) of the surface is 4.6-4.9 μm.

6. A method of producing a developing roller comprising a shaft, an elastic layer formed on an outer periphery of the shaft, and a surface covering layer formed on an outer peripheral face of the elastic layer, wherein a JIS 10-point average roughness (Rz) of the surface is 4-7 μm and a specular gloss at 85° according to JIS Z8741 of the surface is 14-55, the method comprising:

preparing a paint inclusive of a component constituting a surface covering layer, and leaving the paint at room temperature and normal humidity for not less than 24 hours, and thereafter applying the paint onto an outer peripheral face of an elastic layer.

Assignments (2)
ABSORPTION-TYPE COMPANY SPLIT Recorded Aug 26, 2022
From: BRIDGESTONE CORPORATION
To: ARCHEM INC.
Reel/Frame 061328/0297 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 4, 2007
From: YAMAKAWA, KOJI
To: BRIDGESTONE CORPORATION
Reel/Frame 019408/0291 →
Priority Claims (1)
JP 2006-103240 · Apr 4, 2006 · national
Continuity (1)
Related Publication 20080013985A1 · Jan 17, 2008