IP Library Granted Patent US 8,038,791
Granted Patent B2
US 8,038,791 · App. 11/767,614 · Granted Oct 18, 2011

Clinker, system and method for manufacturing the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,038,791
App. No.
11/767,614
Granted
Oct 18, 2011
Kind
B2
Abstract

A cement product is disclosed. The cement product includes clinker defined by a feedstock material and a ladle metallurgical facility slag material derived from a ladle metallurgical facility steel production system. A system and method for manufacturing clinker is also disclosed.

Claims (22)

1. A method for manufacturing a cement product, comprising the steps of:

providing a system for forming clinker, wherein the system consists of:

a controller,

a first variable-speed conveyor belt and a second variable-speed conveyor belt, wherein the controller is communicatively-coupled to each of the first and second variable-speed conveyor belts for controlling the speed of each of the first and second variable-speed conveyor belts,

a rotary kiln including a feed-end and a heat-end, wherein the first and second variable-speed conveyor belts are in communication with the feed-end of the rotary kiln, and

a fuel source in communication with the heat-end, wherein the fuel source provides fuel that is burned for creating a flame within the rotary kiln, wherein the flame is utilized for heating a portion of an interior of the rotary kiln, wherein the portion of the interior of the rotary kiln that is heated by the flame results in the portion of the interior of the rotary kiln forming a sintering zone;

deriving clinker ingredients including a first material comprising a clinker feedstock material, and a second material consisting of a ladle metallurgical facility slag produced by a ladle metallurgical facility steel production system;

delivering a proportion of the clinker feedstock material to the ladle metallurgical facility slag to the feed-end of the rotary kiln by: conveying, with the first variable-speed conveyor belt, the clinker feedstock material to the feed-end of the rotary kiln at a first conveying speed and conveying, with the second variable-speed conveyor belt, the ladle metallurgical facility slag to the feed-end of the rotary kiln at a second conveying speed, wherein the second conveying speed is less than the first conveying speed, wherein the clinker feedstock material and the ladle metallurgical facility slag forms a stream of clinker ingredients; and

directing the stream of clinker ingredients from the feed-end, through the rotary kiln, past the flame and out of the heat-end, and, as the stream of clinker ingredients is directed past the flame, the flame is utilized for heating the stream of clinker ingredients.

2. The method according to claim 1 , wherein after the deriving a ladle metallurgical facility slag step, further comprising the steps of:

crushing the ladle metallurgical facility slag; and

screening the ladle metallurgical facility slag.

3. The method according to claim 1 , wherein after deriving the clinker feedstock material step, further comprising the step of:

grinding the clinker feedstock material.

4. The method according to claim 1 , wherein prior to the delivering step, further comprising the step of:

pre-heating one or more of the clinker feedstock material and ladle metallurgical facility slag.

5. The method according to claim 1 , wherein the second conveying speed is less than the first conveying speed such that the delivered proportion of the clinker feedstock material to the ladle metallurgical facility slag results in the ladle metallurgical facility slag composing approximately 1% to 12% of the stream of clinker ingredients.

6. The method according to claim 1 , wherein the feedstock material includes one or more of a combination selected from a group consisting of

limestone,

clay, and

sand.

7. The method according to claim 1 , wherein the second conveying speed is approximately 1/10 of that of the first conveying speed.