IP Library Granted Patent US 7,820,075
Granted Patent B2
US 7,820,075 · App. 11/805,808 · Granted Oct 26, 2010

Phosphor composition with self-adjusting chromaticity

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,820,075
App. No.
11/805,808
Granted
Oct 26, 2010
Kind
B2
Abstract

Disclosed herein are “smart” phosphor compositions capable of regulating the chromaticity of their emission to substantially constant values even with variations in the excitation radiation they receive to induce photoluminescence. One phosphor of the smart composition demonstrates an increase in emission intensity increases as the wavelength of the excitation radiation is increased. The other phosphor shows a decrease in emission intensity with increasing excitation wavelength. Constant chromaticity in this context is defined as a change in CIE x or y coordinate of less than about five percent over a 10 nm range of excitation wavelengths.

Claims (8)

1. A phosphor composition with self-adjusting chromaticity, the composition comprising:

a first phosphor configured such that its emission intensity increases with increasing excitation wavelength; and

a second phosphor configured such that its emission intensity decreases with increasing excitation wavelength;

wherein the first phosphor is a silicate-based orange phosphor selected from the group consisting of Sr 3 Eu 0.06 Si 1.02 O 5 (F,Cl) 0.18 , Sr 2.94 Ba 0.06 Eu 0.06 Si 1.02 O 5 (F,Cl) 0.18 , and (Sr 0.9 Ba 0.1 ) 2.76 Eu 0.06 Si 1.02 O 5 (F,Cl) 0.18 .

2. A phosphor composition with self-adjusting chromaticity, the composition comprising:

a first phosphor configured such that its emission intensity increases with increasing excitation wavelength; and

a second phosphor configured such that its emission intensity decreases with increasing excitation wavelength;

wherein the second phosphor is a silicate-based green phosphor selected from the group consisting of Sr 0.925 Ba 1.025 Mg 0.05 Eu 0.06 Si 1.03 O 4 (F,Cl) 0.12 , Sr 1.025 Ba 0.925 Mg 0.05 Eu 0.06 Si 1.03 O 4 (F,Cl) 0.12 , and Sr 1.125 Ba 0.825 Mg 0.05 Eu 0.06 Si 1.03 O 4 (F,Cl) 0.12 .

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Apr 14, 2022
From: EAST WEST BANK
To: INTEMATIX HONG KONG CO. LIMITED; INTEMATIX CORPORATION
Reel/Frame 059910/0304 →
SECURITY INTEREST Recorded Oct 27, 2015
From: INTEMATIX HONG KONG CO. LIMITED; INTEMATIX CORPORATION
To: EAST WEST BANK
Reel/Frame 036967/0623 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 5, 2007
From: LI, YI-QUN; DONG, YI
To: INTEMATIX CORPORATION
Reel/Frame 019783/0782 →