IP Library Granted Patent US 9,093,707
Granted Patent B2
US 9,093,707 · App. 11/816,730 · Granted Jul 28, 2015

MultiLayer solid electrolyte for lithium thin film batteries

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,093,707
App. No.
11/816,730
Granted
Jul 28, 2015
Kind
B2
Abstract

A lithium metal thin-film battery composite structure is provided that includes a combination of a thin, stable, solid electrolyte layer [ 18] such as Lipon, designed in use to be in contact with a lithium metal anode layer; and a rapid-deposit solid electrolyte layer [ 16] such as LiAlF 4 in contact with the thin, stable, solid electrolyte layer [ 18 ]. Batteries made up of or containing these structures are more efficient to produce than other lithium metal batteries that use only a single solid electrolyte. They are also more resistant to stress and strain than batteries made using layers of only the stable, solid electrolyte materials. Furthermore, lithium anode batteries as disclosed herein are useful as rechargeable batteries.

Claims (26)

1. A rechargeable lithium battery device comprising:

an anode current collector comprising a metal material selected from copper, nickel, chrome ferrous alloy, a refractory metal, or stainless steel, the metal material being substantially inert toward a lithium metal material;

an anode overlaying the anode current collector, and the anode being electrically coupled to the current collector and comprising lithium metal material;

a first electrolyte layer overlaying the anode consisting of Li 2 S, Li 2 O, or combinations thereof, the first electrolyte layer being substantially stable toward lithium metal material, the first electrolyte layer being characterized by a first deposition rate and a thickness of 10-100 nm;

a second electrolyte layer in direct contact with the first electrolyte layer and comprising at least one of lithium nitride, lithium fluoride, or lithium aluminum fluoride, the second electrolyte layer being characterized by a second deposition rate;

a cathode overlaying the second electrolyte layer; and

a cathode current collector overlaying the cathode;

wherein the first electrolyte layer and the second electrolyte layer are characterized by a total thickness of less than 20 um.

2. The device of claim 1 wherein the anode current collector is characterized by a thickness of about 50-500 nm.

3. The device of claim 1 wherein the anode current collector further comprises a non-conductive substrate material, the metal material overlaying a surface of the non-conductive substrate material.

4. The device of claim 1 wherein the metal material comprises a transition metal material.

5. The device of claim 1 wherein the first electrolyte layer being useful for up to 1000 cycles.

6. The device of claim 1 wherein the first deposition rate is from about 5 nm/min to about 15 nm/min.

7. The device of claim 1 wherein the first electrolyte layer is formed by a vapor deposition process.

8. The device of claim 1 wherein the second electrolyte layer further comprises a polymer material.

9. The device of claim 8 wherein the cathode comprises material selected from lithium vanadate, lithium manganate, lithium nickelate, lithium cobaltate, lithium molybdenum oxide, or lithium titanium oxide.

10. The device of claim 1 wherein the cathode is characterized by a thickness of about 50 nm to about 5000 nm.

11. The device of claim 1 wherein the cathode is formed by deposition on the cathode current collector.

12. The device of claim 1 wherein the cathode current collector comprises at least one of copper, aluminum, gold, chrome ferrous alloy, or refractory metals.

13. The device of claim 1 wherein the cathode current collector is characterized by a thickness of about 50-500 nm.

14. The device of claim 1 wherein the second electrolyte layer is formed by a rapid deposition process.

15. The device of claim 1 wherein the second electrolyte layer further comprises at least one of a polyether, a polyimine, a polythioether, a polyphosphazene, or a polymer blend.

16. The device of claim 1 wherein the second electrolyte layer is substantially free from liquid.

17. The device of claim 1 wherein the second deposition rate is about 1000 nm/min.

18. The device of claim 1 wherein the second electrolyte layer being characterized by a thickness of 650-1000 nm.

19. The device of claim 1 wherein the second deposition rate is higher than the first deposition rate.

Assignments (4)
CHANGE OF NAME Recorded Dec 16, 2025
From: ALLIANCE FOR SUSTAINABLE ENERGY, LLC
To: ALLIANCE FOR ENERGY INNOVATION, LLC
Reel/Frame 073993/0276 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 30, 2008
From: MIDWEST RESEARCH INSTITUTE
To: ALLIANCE FOR SUSTAINABLE ENERGY, LLC
Reel/Frame 021603/0337 →
CONFIRMATORY LICENSE Recorded Oct 3, 2007
From: MIDWEST RESEARCH INSTITUTE
To: ENERGY, UNITED STATES DEPARTMENT OF
Reel/Frame 019916/0827 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 21, 2007
From: LEE, SE-HEE, MR.; TRACY, C. EDWIN, MR.; PITTS, JOHN ROLAND, MR.; LIU, PING
To: MIDWEST RESEARCH INSTITUTE
Reel/Frame 019721/0960 →