IP Library Granted Patent US 7,592,080
Granted Patent B2
US 7,592,080 · App. 11/907,118 · Granted Sep 22, 2009

Perpendicular magnetic recording medium

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,592,080
App. No.
11/907,118
Granted
Sep 22, 2009
Kind
B2
Abstract

A perpendicular magnetic recording medium includes a nonmagnetic substrate; a first underlayer provided on the nonmagnetic substrate; a first nonmagnetic intermediate layer provided on the first underlayer; a second underlayer provided on the first nonmagnetic intermediate layer; a second nonmagnetic intermediate layer provided on the second underlayer; and a magnetic recording layer provided on the second nonmagnetic intermediate layer, wherein the first underlayer comprises a soft magnetic material which has a face-centered cubic structure and which includes at least Ni and Fe, and wherein the second underlayer comprises a soft magnetic material which has a face-centered cubic structure and which includes at least Co. The orientation dispersion is reduced and crystal grain diameters are smaller in the magnetic recording layer, and the film thickness of nonmagnetic intermediate layers can be decreased so that performance improvements such as reduced noise, increased S/N ratio, and improved write-ability are achieved.

Claims (24)

1. A perpendicular magnetic recording medium, comprising:

a nonmagnetic substrate;

a first underlayer provided on the nonmagnetic substrate;

a first nonmagnetic intermediate layer provided on the first underlayer;

a second underlayer provided on the first nonmagnetic intermediate layer;

a second nonmagnetic intermediate layer provided on the second underlayer; and

a magnetic recording layer provided on the second nonmagnetic intermediate layer,

wherein the first underlayer comprises a soft magnetic material which has a face-centered cubic structure and which includes at least Ni and Fe, and

wherein the second underlayer comprises a soft magnetic material which has a face-centered cubic structure and which includes at least Co.

2. The perpendicular magnetic recording medium according to claim 1 , wherein the first underlayer comprises 30-88 at % Ni and 0.1-22 at % Fe where the total number of atoms constituting the first underlayer is taken as reference.

3. The perpendicular magnetic recording medium according to claim 1 , wherein the first underlayer further comprises at least one material selected from the group consisting of Co, Si, B, Nb, N, Ta, Al, Pd, Cr, and Mo.

4. The perpendicular magnetic recording medium according to claim 1 , wherein the first nonmagnetic intermediate layer includes a metal selected from the group consisting of V, Cr, Cu, Nb, Mo, Ru, Rh, Ta, W, Re, and Ir, or an alloy having a main constituent which is at least one metal selected from the group consisting of V, Cr, Cu, Nb, Mo, Ru, Rh, Ta, W, Re, and Ir.

5. The perpendicular magnetic recording medium according to claim 1 , wherein the first nonmagnetic intermediate layer comprises a nonmagnetic alloy including at least Co.

6. The perpendicular magnetic recording medium according to claim 1 , wherein the first nonmagnetic intermediate layer has a thickness ranging between 0.1 nm and 2 nm.

7. The perpendicular magnetic recording medium according to claim 1 , wherein the first nonmagnetic intermediate layer has a thickness ranging between 3 nm and 15 nm.

8. The perpendicular magnetic recording medium according to claim 1 , wherein the second underlayer further comprises at least one material selected from the group consisting of Fe, B, Al, Zr, Mg, and Si.

9. The perpendicular magnetic recording medium according to claim 8 , wherein the second underlayer comprises 10 at % or less Fe, 50 at % or less B, 40 at % or less Al, 15 at % or less Zr, 52 at % or less Mg, or 33 at % or less Si where the total number of atoms constituting the second underlayer is taken as reference.

10. The perpendicular magnetic recording medium according to claim 1 , wherein the second underlayer further comprises one of O or N.

11. The perpendicular magnetic recording medium according to claim 1 , wherein the second nonmagnetic intermediate layer comprises one of Ru or a Ru-base alloy.

12. The perpendicular magnetic recording medium according to claim 1 , wherein the second nonmagnetic intermediate layer has a thickness ranging between 0.1 nm and 20 nm.

13. The perpendicular magnetic recording medium according to claim 1 , wherein the magnetic recording layer comprises a material having a granular structure in which magnetic crystal grains are dispersed in a matrix comprised of one of a nonmagnetic oxide or a nonmagnetic nitride.

14. The perpendicular magnetic recording medium according to claim 1 , further comprising a soft magnetic backing layer provided between the nonmagnetic substrate and the first underlayer.

15. The perpendicular magnetic recording medium according to claim 1 , further comprising a protective film provided on the magnetic recording layer.

16. The perpendicular magnetic recording medium according to claim 1 , further comprising a liquid lubricant layer provided on the protective film.

Assignments (3)
CHANGE OF NAME Recorded Oct 10, 2011
From: FUJI ELECTRIC DEVICE TECHNOLOGY CO., LTD.
To: FUJI ELECTRIC CO., LTD.
Reel/Frame 027249/0159 →
MERGER Recorded Oct 10, 2011
From: FUJI ELECTRIC DEVICE TECHNOLOGY CO., LTD. (MERGER)
To: FUJI ELECTRIC CO., LTD.
Reel/Frame 027288/0820 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 7, 2008
From: TAKENOIRI, SHUNJI; SAKAI, YASUSHI
To: FUJI ELECTRIC DEVICE TECHNOLOGY CO., LTD.
Reel/Frame 020357/0064 →