IP Library Granted Patent US 8,323,849
Granted Patent B2
US 8,323,849 · App. 11/947,011 · Granted Dec 4, 2012

Electrolyte membrane containing a crosslinked polybenzoxazine-based compound for fuel cell and fuel cell using the same

Assignee: Samsung Electronics Co., Ltd.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,323,849
App. No.
11/947,011
Granted
Dec 4, 2012
Kind
B2
Abstract

A fuel cell including an electrolyte membrane and/or an electrode which includes a crosslinked polybenzoxazine-based compound formed of a polymerized product of at least one selected from a first benzoxazine-based monomer and second benzoxazine-based monomer, the first benzoxazine-based monomer and second benzoxazine-based monomer having a halogen atom or a halogen atom-containing functional group, crosslinked with a cross-linkable compound.

Claims (42)

1. An electrolyte membrane for a fuel cell, comprising:

a crosslinked polybenzoxazine-based compound formed of a benzoxazine-based monomer represented by Formula 1 below crosslinked with a cross-linkable compound,

wherein R 1 is a halogen atom, and R 2 through R 4 are hydrogen, and

R 5 is an aryl group selected from groups represented by the formulae below:

2. A fuel cell comprising:

a cathode;

an anode; and

an electrolyte membrane disposed between the cathode and the anode,

wherein the electrolyte membrane comprises a crosslinked polybenzoxazine-based compound formed of at least one monomer selected from a first benzoxazine-based monomer represented by Formula 1 or Formula 3 below cross-linked with a cross-linkable compound and a second benzoxazine-based monomer represented by Formula 5 below crosslinked with a cross-linkable compound,

wherein R1 is a halogen atom, and R2 through R4 are hydrogen, R5 is an aryl group selected from groups represented by the formulae below:

wherein at least one of the anode and the cathode comprises a catalyst layer comprising a polymer of a benzoxazine-based monomer represented by Formula 4 below.

3. The fuel cell of claim 2 , wherein the catalyst layer further comprises at least one binder selected from the group consisting of poly(vinylidenefluoride), polytetrafluoroethylene (PTFE), a tetrafluoroethylene-hexafluoroethylene copolymer, fluorinated ethylene propylene (FEP), styrene butadiene rubber (SBR), and polyurethane.

4. The fuel cell of claim 2 , wherein an amount of the binder is in the range of 0.1 to 50 parts by weight based on 100 parts by weight of the catalyst.

5. The fuel cell of claim 2 , wherein the catalyst layer further comprises a proton conductor.

6. The fuel cell of claim 5 , wherein the proton conductor is a phosphoric acid or a C 1 -C 20 organic phosphonic acid.

7. The fuel cell of claim 2 , wherein an amount of the polymer of at least one selected benzoxazine-based monomer of the polymer of the at least one of the cathode and the anode is in the range of 0.1 to 50 parts by weight based on 100 parts by weight of the catalyst.

8. The fuel cell of claim 2 , wherein the first benzoxazine-based monomer represented by Formula 1 is a benzoxazine-based monomer represented by Formula 4

9. An electrolyte membrane for a fuel cell, which comprises a crosslinked polybenzoxazine-based compound formed of a benzoxazine-based monomer represented by Formula 4 below crosslinked with a cross-linkable compound

10. The electrolyte membrane of claim 9 , wherein the cross-linkable compound is at least one selected from the group consisting of polybenzimidazoles (PBI), a polybenzimidazole-base complex, polybenzthiazoles, polybenzoxazoles, and polyimides.

11. The electrolyte membrane of claim 9 , wherein an amount of the cross-linkable compound is in the range of 5 to 95 parts by weight based on 100 parts by weight of the total weight of at least one selected from the first benzoxazine-based monomer and the second benzoxazine-based monomer.

12. The electrolyte membrane of claim 9 , further comprising a proton conductor.

13. The electrolyte membrane of claim 12 , wherein the proton conductor is a phosphoric acid or a C 1 -C 20 organic phosphonic acid.

14. A fuel cell comprising:

a cathode;

an anode; and

the electrolyte membrane according to claim 9 disposed between the cathode and the anode.

15. The fuel cell of claim 14 , wherein the catalyst layer further comprises at least one binder selected from the group consisting of poly(vinylidenefluoride), polytetrafluoroethylene (PTFE), a tetrafluoroethylene-hexafluoroethylene copolymer, fluorinated ethylene propylene (FEP), styrene butadiene rubber (SBR), and polyurethane.

16. The fuel cell of claim 15 , wherein an amount of the binder is in the range of 0.1 to 50 parts by weight based on 100 parts by weight of the catalyst.

17. The fuel cell of claim 15 , wherein the catalyst layer further comprises a proton conductor.

18. The fuel cell of claim 17 , wherein the proton conductor is a phosphoric acid or a C 1 -C 20 organic phosphonic acid.

19. The fuel cell of claim 14 , wherein an amount of the polymer of at least one selected benzoxazine-based monomer of the polymer of the at least one of the cathode and the anode is in the range of 0.1 to 50 parts by weight based on 100 parts by weight of the catalyst.

20. A fuel cell comprising:

a cathode;

an anode; and

an electrolyte membrane disposed between the cathode and the anode,

wherein the electrolyte membrane comprises a crosslinked polybenzoxazine-based compound formed of a benzoxazine-based monomer represented by Formula 3 below crosslinked with a cross-linkable compound,

and wherein at least one of the anode and the cathode comprises a catalyst and a polymer of a benzoxazine-based monomer represented by Formula 4 below.

21. The fuel cell of claim 20 , wherein the catalyst layer further comprises at least one binder selected from the group consisting of poly(vinylidenefluoride), polytetrafluoroethylene (PTFE), a tetrafluoroethylene-hexafluoroethylene copolymer, fluorinated ethylene propylene (FEP), styrene butadiene rubber (SBR), and polyurethane.

22. The fuel cell of claim 20 , wherein an amount of the binder is in the range of 0.1 to 50 parts by weight based on 100 parts by weight of the catalyst.

23. The fuel cell of claim 20 , wherein the catalyst layer further comprises a proton conductor.

24. The fuel cell of claim 23 , wherein the proton conductor is a phosphoric acid or a C 1 -C 20 organic phosphonic acid.

25. The fuel cell of claim 20 , wherein an amount of the polymer of at least one selected benzoxazine-based monomer of the polymer of the at least one of the cathode and the anode is in the range of 0.1 to 50 parts by weight based on 100 parts by weight of the catalyst.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 3, 2007
From: CHOI, SEONG-WOO; PARK, JUNG-OCK
To: SAMSUNG ELECTRONICS CO., LTD.
Reel/Frame 020216/0977 →
Priority Claims (1)
KR 10-2007-0111588 · Nov 2, 2007 · national
Continuity (1)
Related Publication 20090117436A1 · May 7, 2009