IP Library Patent Application 11978213
Patent Application
App. No. 11/978,213

Method for manufacturing nickel zinc batteries

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
11/978,213
Abstract

Methods of manufacturing a rechargeable power cell are described. Methods include providing a slurry, paste, or dry mixture of negative electrode materials having low toxicity and including dispersants to prevent the agglomeration of particles that may adversely affect the performance of power cells. The methods utilize semi-permeable sheets to separate the electrodes and minimize formation of dendrites; and further provide electrode specific electrolyte to achieve efficient electrochemistry and to further discourage dendritic growth in the cell. The negative electrode materials may be comprised of zinc and zinc compounds. Zinc and zinc compounds are notably less toxic than the cadmium used in nickel cadmium batteries. The described methods may utilize some production techniques employed in existing NiCad production lines. Thus, the methods described will find particular use in an already well-defined and mature manufacturing base.

Claims (7)

1 . A method of manufacturing a rechargeable power cell, said method comprising:

applying a zinc negative electrode material to a first conductive carrier to form a first electrode sheet;

applying a nickel positive electrode material to a second conductive carrier to form a second electrode sheet;

disposing at least one separator sheet between the first electrode sheet and the second electrode sheet such that the first electrode and the second electrode sheets and the at least one separator sheet form are layered to form a cell assembly;

winding or folding the cell assembly to form a three-dimensional structure having a form factor generally corresponding with that of the rechargeable power cell; and

electrically connecting a copper negative internal terminal to the negative electrode of the cell assembly,

wherein the power cell exhibits an overall impedance of approximately 3 to 5 milliohms.

Assignments (2)
RELEASE OF SECURITY INTEREST Recorded Nov 15, 2016
From: COMERICA BANK, AS AGENT
To: POWERGENIX SYSTEMS, INC.
Reel/Frame 040622/0032 →
SECURITY AGREEMENT Recorded Oct 31, 2011
From: POWERGENIX SYSTEMS, INC.
To: COMERICA BANK
Reel/Frame 027150/0001 →