IP Library Granted Patent US 8,039,097
Granted Patent B2
US 8,039,097 · App. 11/983,487 · Granted Oct 18, 2011

Methods for protecting patinated surfaces of copper products and patinated copper product

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,039,097
App. No.
11/983,487
Granted
Oct 18, 2011
Kind
B2
Abstract

A method for the temporary protection of patinated surfaces of copper products, in which an aqueous polymer dispersion is applied to the patinated surface, so that the polymer dispersion penetrates regions of the porous patina that are close to the surface, and in which the aqueous polymer dispersion is subsequently dried, so that it forms a composite with the patina that is permeable to water vapor diffusion. The polymer dispersion binds loose dust located on prepatinated copper products and simplifies the handling of the copper products. It behaves in a hydrophobic manner, but on the other hand it permits the required access of air moisture and water to the patina layer for further weathering.

Claims (13)

1. A composite material comprising an aqueous polymer dispersion, a copper product having a patinated surface and regions of a porous patina that are close to the surface, the regions of porous patina close to the surface comprising a plurality of open pores, each having a wall and being reinforced with an aqueous polymer dispersion, wherein the composite material is permeable to water vapor diffusion, wherein the polymer dispersion effloresces over time, and provides temporary protection, wherein the aqueous polymer dispersion has a proportion of solid between 15% and 20%, and wherein the solid only deposits on the walls of the open pores without completely filling up the pores.

2. The composite material according to claim 1 , wherein the aqueous polymer dispersion is visually neutral compared to the patina.

3. The composite material according to claim 1 , wherein a quantity of 5 g/m 2 to 10 g/m 2 of the aqueous polymer dispersion is applied to the patinated surface.

4. The composite material according to claim 1 , wherein the aqueous polymer dispersion is based on acrylate.

5. The composite material according to claim 1 , wherein the aqueous polymer dispersion is free of solvent.

6. A method for forming the composite material according to claim 1 , comprising:

applying the aqueous polymer dispersion to the patinated surface, so that the polymer dispersion penetrates regions of porous patina that are close to the surface, and subsequently drying the aqueous polymer dispersion.

7. The method according to claim 6 , wherein a quantity of 5 g/m 2 to 10 g/m 2 of the aqueous polymer dispersion is applied to the patinated surface.

8. The method according to claim 7 , wherein the aqueous polymer dispersion is applied to the patinated surface in the form of drops.

9. The method according to claim 7 , wherein the water of the applied polymer dispersion is evaporated with the aid of infrared radiation.

10. The method according to claim 6 , wherein the aqueous polymer dispersion is applied to the patinated surface in the form of drops.

11. The method according to claim 10 , wherein the water of the applied polymer dispersion is evaporated with the aid of infrared radiation.

12. The method according to claim 6 , wherein the water of the applied polymer dispersion is evaporated with the aid of infrared radiation.

Assignments (3)
MERGER Recorded Jul 30, 2015
From: KME GERMANY AG
To: KME GERMANY AG & CO. KG
Reel/Frame 036233/0665 →
CHANGE OF NAME Recorded Jul 30, 2015
From: KME GERMANY AG & CO. KG
To: KME GERMANY GMBH & CO. KG
Reel/Frame 036234/0062 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 15, 2008
From: HOVELING, STEFAN
To: KME GERMANY AG
Reel/Frame 020538/0206 →