Method of making cathode
View Patent ↗A method of making a cathode for a lithium primary battery includes lithiated manganese dioxide and a carbon fluoride. The cathode can provide high capacity and voltage with low gassing.
1. A method of making a primary lithium battery comprising a cathode including cathode active material, comprising
(a) blending a lithiated manganese dioxide and a carbon fluoride to provide a cathode mixture including the lithiated manganese dioxide and the carbon fluoride in a specific weight ratio;
(b) using the cathode mixture to form a cathode adjacent a first surface of a separator, wherein the only cathode active material in the cathode consists of the lithiated manganese dioxide and the carbon fluoride in the specific weight ratio;
(c) providing an anode adjacent to a second surface of the separator;
(d) assembling the cathode, separator, and anode into a cylindrical housing to provide the primary lithium battery, and wherein the lithiated manganese dioxide has a specific surface area of between 10.0 m 2 /g and 20.0 m 2 /g.
2. The method material of claim 1 , wherein the lithiated manganese dioxide and the carbon fluoride are present in a ratio in the range of 20:80 to 80:20 by weight.
3. The method of claim 1 , wherein step (a) comprises blending the carbon fluoride, the lithiated manganese dioxide, and a carbon source to provide the cathode mixture.