Rare earth sintered magnet and method for producing same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,182,618
App. No.
12/095,617
Granted
May 22, 2012
Kind
B2
Abstract

A sintered rare-earth magnet includes an Nd 2 Fe 14 B type crystalline phase as its main phase and Al as an additive. The magnet includes at least one light rare-earth element LR selected from the group consisting of yttrium and the rare-earth elements other than Dy, Ho and Tb, and at least one heavy rare-earth element HR selected from the group consisting of Dy, Ho and Tb. The mole fractions α1, α2 and β of the light and heavy rare-earth elements LR and HR and Al satisfy the inequalities 25≦α1+α2≦40 mass %, 0<α2≦40 mass %, β>0.20 mass %, and 0.04≦β/α2≦0.12.

Claims (16)

1. A sintered rare-earth magnet comprising an Nd 2 Fe 14 B type crystalline phase as its main phase and Al as an additive; wherein

the rare-earth magnet includes at least one light rare-earth element LR selected from the group consisting of yttrium and the rare-earth elements other than Dy, Ho and Tb, and at least one heavy rare-earth element HR selected from the group consisting of Dy, Ho and Tb; and

α1, α2 and β of the light and heavy rare-earth elements LR and HR and Al satisfy the inequalities

25≦α1+α2≦40 mass %,

4.0≦α2≦40 mass %,

β≧0.35 mass %, and

0.04≦β/α2≦0.12; and

the rare-earth magnet further includes 0.01 to 0.2 mass % of at least one additive element M that is selected from the group consisting of Si, Ti, V, Cr, Mn, Ni, Cu, Zn, Ga, Zr, Nb, Mo, Ag, In, Sn, Hf, Ta, W, Pb and Bi.

2. The sintered rare-earth magnet of claim 1 , wherein the magnet is made of a sintered powder of a rapidly solidified alloy that has been obtained by a strip casting process.

3. A method for producing a sintered rare-earth magnet, the method comprising the steps of:

providing a rapidly solidified alloy that includes at least one light rare-earth element LR, at least one heavy rare-earth element HR and Al as an additive, the at least one light rare-earth element LR being selected from the group consisting of yttrium and the rare-earth elements other than Dy, Ho and Tb, the at least one heavy rare-earth element HR being selected from the group consisting of Dy, Ho and Tb, α1, α2 and β of the light and heavy rare-earth elements LR and HR and Al satisfying the inequalities 25≦α1+α2≦40 mass %, 4.0≦α2≦40 mass %, β≧0.35 mass %, and 0 04≦β/α2≦0.12;

pulverizing the rapidly solidified alloy to make a powder;

compacting the powder under a magnetic field to make a compact; and

sintering the compact, thereby obtaining a sintered rare-earth magnet including an Nd 2 Fe 14 B type crystalline phase as its main phase; wherein

the rapidly solidified alloy includes 0.01 to 0.2 mass % of at least one additive element M that is selected from the group consisting of Si, Ti, V, Cr, Mn, Ni, Cu, Zn, Ga, Zr, Nb, Mo, Ag, In, Sn, Hf, Ta, W, Pb and Bi.

4. The method of claim 3 , wherein the step of providing a rapidly solidified alloy includes quenching a melt of a material alloy by a strip casting process.

Assignments (3)
NUNC PRO TUNC ASSIGNMENT Recorded Jun 3, 2024
From: HITACHI METALS, LTD.
To: HITACHI, LTD.
Reel/Frame 067605/0821 →
CHANGE OF NAME Recorded Dec 27, 2023
From: HITACHI METALS, LTD.
To: PROTERIAL, LTD.
Reel/Frame 066130/0563 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 30, 2008
From: NOZAWA, NORIYUKI; ODAKA, TOMOORI; MATSUURA, YUTAKA
To: HITACHI METALS, LTD.
Reel/Frame 021022/0310 →