IP Library Granted Patent US 8,685,117
Granted Patent B2
US 8,685,117 · App. 12/096,352 · Granted Apr 1, 2014

Lithium metal foil for battery or capacitor

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,685,117
App. No.
12/096,352
Granted
Apr 1, 2014
Kind
B2
Abstract

A lithium ion capacitor includes, as a lithium ion supply source, a lithium metal foil for batteries or capacitors. A current collector 4 and a separator 3 formed of a paper or resin nonwoven fabric are preliminarily pressure-bonded and integrated to opposite surfaces of a lithium metal foil 1 for batteries or capacitors.

Claims (14)

1. A method of manufacturing strip-shaped lithium metal foils for batteries or capacitors comprising:

attaching a separator to one surface of a lithium metal foil by pressure-bonding;

attaching a current collector to an opposite surface of the lithium metal foil by pressure-bonding, so as to form an attached lithium metal foil; wherein the attached lithium metal foil consists of the lithium metal foil, the separator, and the current collector;

cutting the attached lithium metal foil in which the separator is attached on the one surface by pressure-bonding and the current collector is attached on the opposite surface by pressure-bonding to form the strip-shaped lithium metal foils; and

disposing the strip-shaped lithium metal foils into cells of the batteries or capacitors.

2. The manufacturing method according to claim 1 ,

wherein the separator and the current collector are porous materials having through-holes.

3. The manufacturing method according to claim 1 ,

wherein the separator is a paper or resin non-woven fabric, and

wherein the paper or resin non-woven fabric is attached to the lithium metal foil by pressure-bonding.

4. The manufacturing method according to claim 1 ,

wherein the lithium metal foil has a thickness of 5 to 500 μm.

5. The manufacturing method according to claim 1 ,

wherein the separator and the current collector have a thickness of 10 to 150 μm.

Assignments (1)
CHANGE OF ADDRESS Recorded Nov 12, 2014
From: FUJI JUKOGYO KABUSHIKI KAISHA
To: FUJI JUKOGYO KABUSHIKI KAISHA
Reel/Frame 034215/0580 →