IP Library Granted Patent US 8,479,478
Granted Patent B2
US 8,479,478 · App. 12/122,322 · Granted Jul 9, 2013

Surface-treated multi-layered polymer film

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,479,478
App. No.
12/122,322
Granted
Jul 9, 2013
Kind
B2
Abstract

A sealable polymeric film structure comprising (a) a core layer including a thermoplastic polymer, the core layer having a machine side and a product side that is on a side of the film opposite from the machine side; and (b) a sealable skin layer positioned on the product side of the core layer, the sealable skin layer including a thermoplastic polymer, wherein an exterior surface of the sealable skin layer has a receding Cahn value of at least about 0.48; and wherein in some heat—sealable embodiments, the sealable skin layer sealed to itself has a MST of from about 175° F. to about 220° F., with a jaw pressure of 20 psi for 0.75 seconds and a minimum acceptable seal strength of 200 g/in at 175° F., on a Wrap-Ade™ Crimp Sealer Model J or K.

Claims (24)

1. A method of packaging a product within a heat-sealable polymeric film on a packaging machine, the method comprising the steps of:

(a) drawing the heat-sealable polymeric film structure through the packaging machine from an inlet side of the packaging machine to an outlet side of the packaging machine, the heat-sealable polymeric film structure having a product side and a machine side, the heat-sealable polymeric film structure comprising:

(i) a core layer having a machine side and a product side opposite from the machine side, wherein the core layer comprises a polymer matrix and optionally a cavitating agent;

(ii) a heat-sealable skin layer on the product side of the core layer, the heat-sealable skin layer having a product side exterior surface with a product side surface energy having a receding DCA Cahn value of at least about 0.48;

wherein the heat-sealable skin layer comprises a polymer material selected from the group consisting of polyethylene, polybutene, polylactic acid, propylene-ethylene copolymers, propylene-butylene copolymers, propylene-ethylene-butylene terpolymers and ethylene-propylene-butylene terpolymers;

(b) positioning a product on the product side exterior surface of the heat-sealable skin layer;

(c) engaging a first portion of the product side exterior surface of the heat-sealable skin layer with a second portion of the product side exterior surface of the heat-sealable skin layer, whereby a seal area is formed over the engaged portions of the product side exterior surfaces of the heat-sealable skin layers, or

optionally engaging a first portion of the product side exterior surface of the heat-sealable skin layer with a portion of the machine side of the heat-sealable polymeric film structure, whereby a seal area is formed over the engaged portions of the product side exterior surface of the heat-sealable skin layer and the machine side of the heat-sealable polymeric film,

whereby a product space is created within the product side of the heat-sealable polymeric film structure; and

(d) applying heat to at least a portion of the seal area to form a seal and encase at least a portion of the product within the product space,

wherein the seal formed has the following sealing properties: (A) a minimum sealing temperature (MST) of from about 175° F. to about 220° F. with a jaw pressure of 20 psi for 0.75 seconds, and (B) a minimum acceptable seal strength of 200 g/in at 175° F.,

wherein the product is substantially frozen and comprises at least one of water, an aqueous-based product, or dairy-based product.

2. The method of packaging a product of claim 1 , wherein the aqueous-based or dairy-based product comprises at least one of an ice cream treat, a sugar-based treat, a sugar-free treat, and a yogurt treat.

3. The method of packaging a product of claim 1 , wherein at least a portion of the product is adhered on the product side exterior surface of the heat-sealable skin layer when the packaging machine is damp or in a humid environment.

4. The method of packaging a product of claim 3 , wherein the product side exterior surface of the heat-sealable skin layer is surface-treated by one of corona treatment, flame treatment, and plasma treatment.

5. The method of packaging a product of claim 1 , wherein the product side exterior surface of the heat-sealable skin layer is surface-treated by one of corona treatment, flame treatment, and plasma treatment.

6. The method of packaging a product of claim 5 , wherein at least a portion of the product is adhered to the surface-treated product side exterior surface.

7. The method of packaging a product of claim 6 , wherein the sealing properties of the heat-sealable skin layer are maintained following surface treatment.

8. The method of packaging a product of claim 1 , wherein the heat-sealable polymeric film structure of step (a) further comprises (iii) a second skin layer on the machine side of the core layer, the second skin layer having a machine side exterior surface with a machine side surface energy having a receding Cahn value not to exceed 0.20,

wherein the second skin layer is a thermoplastic polymer selected from the group consisting of polypropylene polyethylene polybutylene, polyesters and blends thereof.

9. The method of packaging a product of claim 8 , wherein the machine side surface energy has a receding Cahn value that is negative.

10. The method of packaging a product of claim 8 , wherein at least a portion of the machine side exterior surface is non-water-wet when the packaging machine is damp or in a humid environment.

11. The method of packaging a product of claim 10 , wherein the machine side exterior surface of the second skin layer is surface-treated by one of corona treatment, flame treatment, and plasma treatment.

12. The method of packaging a product of claim 11 , further comprising the step of applying one of a printing ink and a coating composition on at least about 10% of the area of the machine side exterior surface.

Assignments (6)
RELEASE OF SECURITY INTEREST Recorded Jun 17, 2021
From: BANK OF AMERICA, N.A., AS AGENT
To: JINDAL FILMS AMERICAS LLC
Reel/Frame 056616/0092 →
SECURITY INTEREST Recorded Sep 4, 2018
From: JINDAL FILMS AMERICAS LLC
To: BANK OF AMERICA, N.A., AS AGENT
Reel/Frame 047570/0731 →
CHANGE OF NAME Recorded Feb 12, 2014
From: FILMS AMERICAS, LLC
To: JINDAL FILMS AMERICAS LLC
Reel/Frame 032201/0371 →
PURCHASE OF FILMS AMERICAS, LLC Recorded Jan 16, 2014
From: EXXONMOBIL OIL CORPORATION
To: JPF USA LLC
Reel/Frame 032072/0498 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 3, 2014
From: EXXONMOBIL OIL CORPORATION
To: FILMS AMERICAS, LLC
Reel/Frame 031885/0959 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 16, 2008
From: CLECKNER, MICHAEL DALE; WILKINS, SCOTT P.
To: EXXONMOBIL OIL CORPORATION
Reel/Frame 020960/0753 →