IP Library Granted Patent US 7,973,998
Granted Patent B2
US 7,973,998 · App. 12/152,969 · Granted Jul 5, 2011

Temperature activated optical films

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,973,998
App. No.
12/152,969
Granted
Jul 5, 2011
Kind
B2
Abstract

The present invention discloses a multilayer dielectric optical structure wherein one of the optical materials in the multilayer structure shows an optically isotropic state above and a birefringent state below a characteristic temperature Tc near the room temperature. The optical structure reflects a predetermined wavelength range of electromagnetic radiation above the Tc but allow the same to transmit through below the Tc. The predetermined wavelength can be the near infrared radiation from 700 nm to 2500 nm, and the optical structure rejects solar heat in warm summer days but admits the same to interior on a colder winter day.

Claims (32)

1. A multilayer dielectric optical structure, for selectively reflecting a predetermined wavelength, comprising:

a transparent substrate;

a plurality of alternating first layers and second layers on the substrate, wherein the first layers comprise a first optical material having a first optical axis and a first refractive index along the first optical axis, and wherein the second layers comprise a second optical material having a second optical axis and a second refractive index along the second optical axis below a characteristic transition temperature (Tc) and a third refractive index above the Tc, wherein the second optical material includes a liquid crystal material having an isotropic-to-ordered state transition temperature between 15 and 35 degrees Celsius, wherein the first and second optical axes are substantially parallel and the first and second refractive indices are substantially equal, and wherein the third refractive index differs from the second refractive index and from the first refractive index; and

wherein the optical thickness of each of the first layers is equal to ¼ times the predetermined wavelength and the optical thickness of each of the second layers is equal to ¼ times the predetermined wavelength when the temperature is above the Tc.

2. The optical structure of claim 1 , wherein one optical axis of the first layer is parallel to the layer surface.

3. The optical structure of claim 1 , wherein the third refractive index differs from the second refractive index by 0.05 or greater.

4. The optical structure of claim 2 , wherein the first optical material comprises semicrystalline polymers.

5. The optical structure of claim 2 , wherein the first optical material includes polyethylene terephthalate.

6. The optical structure of claim 1 , wherein the first optical material is a photo-polymerizable material.

7. A multilayer dielectric optical structure, for selectively reflecting a predetermined wavelength, comprising:

a transparent substrate;

a plurality of alternating first layers and second layers on the substrate, wherein the first layers comprise a first optical material having a first optical axis and a first refractive index along the first optical axis, and wherein the second layers comprise a second optical material having a second optical axis and a second refractive index along the second optical axis below a characteristic transition temperature (Tc) and a third refractive index above the Tc, wherein the second layer includes a polymer mesh at less than 10 weight % for maintaining mechanical stability and for limiting mobility of a liquid crystal material, wherein the first and second optical axes are substantially parallel and the first and second refractive indices are substantially equal, wherein the third refractive index differs from the second refractive index and from the first refractive index; and

wherein the optical thickness of each of the first layers is equal to ¼ times the predetermined wavelength and the optical thickness of each of the second layers is equal to ¼ times the predetermined wavelength when the temperature is above the Tc.

8. The optical structure of claim 7 , wherein the polymer mesh is substantially the same material as the first optical material.

9. The optical structure of claim 7 , wherein the polymer mesh is a photo-polymerized polymer.

10. The optical structure of claim 7 , wherein the polymer mesh is a thermosetting polymer.

11. The optical structure of claim 1 , wherein the liquid crystal material is in a nematic liquid crystal phase below the Tc and an isotropic phase above the Tc.

12. The optical structure of claim 1 , wherein one optical axis of the first layer is perpendicular to the layer surface and the liquid crystal material is in a discotic liquid crystal phase below the Tc and an isotropic phase above the Tc.

13. The optical structure of claim 1 , wherein the first optical material is isotropic.

14. The optical structure of claim 1 , wherein the number of first layers is between 1 and 1000.

15. The optical structure of claim 1 , wherein the first layer is a stretch-induced optically anisotropic material.

16. A multilayer dielectric optical system, comprising:

a transparent substrate;

a plurality of dielectric pairs, wherein each pair comprises a first layer of a first optical material having a first refractive index and a liquid crystal layer having a third isotropic refractive index when temperature is above a transition temperature, wherein the optical thickness of the first layer equals the optical thickness of the liquid crystal layer which equals ¼ of a predetermined wavelength λ 0 , wherein the number of dielectric pairs is between 1 to 500; and

the optical thickness of each adjacent pair is in accordance to the formula:

d N+1 =r d N

first layer =¼λ 0

where d N is the optical thickness of Nth pair, it is the two times the optical thickness of each layer in the pair and r is a numerical number between 0.85 to 0.999.

17. The optical structure of claim 1 , wherein the second layer includes a polymer mesh at less than 10 weight % for maintaining mechanical stability and for limiting the mobility of the liquid crystal material.

18. The optical structure of claim 17 , wherein the polymer mesh is substantially the same material as the first optical material.

19. The optical structure of claim 17 , wherein the polymer mesh is a photo-polymerized polymer.

20. The optical structure of claim 17 , wherein the polymer mesh is a thermosetting polymer.

Assignments (4)
MERGER Recorded Dec 14, 2011
From: SERIOUS MATERIALS, INC.
To: SERIOUS ENERGY, INC.
Reel/Frame 027379/0410 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 20, 2009
From: NAXELLENT, LLC
To: SERIOUS MATERIALS, INC.
Reel/Frame 023125/0429 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 18, 2009
From: XUE, JIUZHI
To: NAXELLENT, LLC
Reel/Frame 023114/0016 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 21, 2009
From: NAXELLENT, LLC
To: SERIOUS MATERIALS, INC.
Reel/Frame 022574/0832 →