IP Library Granted Patent US 8,481,152
Granted Patent B2
US 8,481,152 · App. 12/191,863 · Granted Jul 9, 2013

Refractory material with improved resistance to molten slag

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,481,152
App. No.
12/191,863
Granted
Jul 9, 2013
Kind
B2
Abstract

A treated refractory material includes a porous refractory material having one or more protective materials disposed within pores of the refractory material. Methods of preparing the treated refractory material are also provided. The treated refractory material provides protection from the penetration of slag and extends the service life of the refractory material.

Claims (19)

1. A material comprising:

a refractory material comprising a crystalline phase; and

a protective material comprising an amorphous phase, wherein the protective material comprises a refractory glass having a melting temperature greater than 700° C.,

wherein the protective material is disposed in pores in the refractory material.

2. The material of claim 1 , wherein the melting temperature of the refractory glass is greater than 1300° C.

3. The material of claim 1 , wherein the protective material comprises enstatite.

4. The material of claim 1 , wherein the refractory material comprises a chromia-alumina sintered brick, a chromia-alumina-phosphate sintered brick, a chromia-zirconia sintered brick, or a chromia-magnesia sintered brick.

5. The material of claim 1 , wherein the protective material fills from about 3 to about 60 percent of the volume of the pores in the refractory material.

6. The material of claim 1 , wherein the protective material comprises a powder.

7. The material of claim 1 , wherein the protective material comprises from about 2 to about 15 percent by volume of the refractory material.

8. The material of claim 1 , wherein the material is disposed on the lining of a gasifier.

9. A material comprising:

a refractory material comprising a crystalline phase, wherein the refractory material comprises a chromia-alumina sintered brick, a chromia-alumina-phosphate sintered brick, a chromia-zirconia sintered brick, a chromia-magnesia sintered brick, or a combination thereof; and

a protective material comprising an amorphous phase, wherein the protective material comprises a refractory glass having a melting temperature greater than 700° C.

10. The material of claim 9 , wherein the melting temperature of the refractory glass is greater than 1300° C.

11. The material of claim 9 , wherein the protective material comprises enstatite.

12. The material of claim 9 , wherein the protective material comprises a powder.

13. The material of claim 9 , wherein the protective material comprises from about 2 to about 15 percent by volume of the refractory material.

14. The material of claim 9 , wherein the material is disposed on the lining of a gasifier.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 22, 2019
From: GENERAL ELECTRIC COMPANY
To: AIR PRODUCTS AND CHEMICALS, INC.
Reel/Frame 050787/0642 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 14, 2008
From: SHUBA, ROMAN; CHEN, WEI; THOMPSON, ANTHONY MARK
To: GENERAL ELECTRIC COMPANY
Reel/Frame 021392/0302 →