IP Library Granted Patent US 8,323,509
Granted Patent B2
US 8,323,509 · App. 12/227,040 · Granted Dec 4, 2012

Rehabilitation method

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,323,509
App. No.
12/227,040
Granted
Dec 4, 2012
Kind
B2
Abstract

A method of rehabilitation of a deposition area to render it suitable for plant growth comprising a particulate mineral material, which particulate mineral material has been dewatered from a suspension of said material, comprising the steps of transferring the suspension of particulate mineral material as a fluid to the deposition area, and in which the suspension is allowed to stand and dewater at the deposition area to form a dewatered particulate mineral material, wherein the rehabilitation of the disposal area is achieved by adding a dewatering amount of a polymer to the suspension of the particulate mineral material while it is being transferred as a fluid to the deposition area, wherein the polymer is either a synthetic water-soluble polymer formed from one or more ethylenically unsaturated monomers having an intrinsic viscosity of at least 4 dl/g or a water-soluble polymer that is a natural polymer or semi natural polymer.

Claims (26)

1. A method of rehabilitation of a deposition area to render it suitable for plant growth comprising a particulate mineral material, which particulate mineral material has been dewatered from a suspension of said material, the method comprising the steps of:

(i) transferring the suspension of particulate mineral material as a fluid to the deposition area, and in which the suspension is allowed to stand and dewater at the deposition area to form a dewatered particulate mineral material;

(ii) rehabilitating the deposition area by adding a dewatering amount of a polymer to the suspension of the particulate mineral material while it is being transferred as a fluid to the deposition area;

(iii) allowing the suspension to form a non-segregated treated stack; and

(iv) introducing into the particulate mineral material prior to rigidification any of plants, seedlings, or seeds suitable for germination,

wherein the polymer is either a synthetic water-soluble polymer formed from one or more ethylenically unsaturated monomers having an intrinsic viscosity of at least 4 dl/g or a water-soluble polymer that is a natural polymer or semi natural polymer, wherein the synthetic polymer is formed from monomer(s) selected from the group consisting of (meth)acrylic acid, allyl sulphonic acid and 2-acrylamido-2-methyl propane sulphonic acid as the free acids or salts thereof, optionally in combination with non-ionic co-monomers, selected from the group consisting of (meth)acrylamide, hydroxyl alkyl esters of (meth)acrylic acid and N-vinyl pyrrolidone, and wherein the polymer is combined with the suspension at a dose of 10 grams to 10,000 grams per tonne of material solids.

2. A method according to claim 1 in which the polymer is a nonionic or anionic polymer of one or more ethylenically unsaturated monomers.

3. A method according to claim 2 in which the polymer is a homopolymer of acrylamide or a copolymer of acrylamide with sodium acrylate.

4. A method according to claim 1 in which the suspension of particulate mineral material is a waste material from a mineral processing operation.

5. A method according to claim 1 in which the suspension of particulate mineral material is transferred along a conduit and through an outlet to the deposition area.

6. A method according to claim 1 in which the suspension of particulate mineral material that has been transferred to the deposition area rigidifies upon standing.

7. A method according to claim 6 in which the suspension of particulate mineral material upon reaching the deposition area flows over the surface of previously rigidified mineral material.

8. A method according to claim 1 in which the suspension of particulate mineral material is transferred by pumping it through a conduit and the polymer is added subsequently to the pumping stage.

9. A method according to claim 1 in which the suspension of particulate mineral material is transferred by pumping it through a conduit and polymer is added during or prior to the pumping stage.

10. A method according to claim 1 in which the suspension of particulate mineral material is transferred through a conduit having an outlet wherein the polymer is added to the suspension as it exits the outlet.

11. A method according to claim 1 in which the suspension of particulate mineral material is transferred through a conduit having an outlet wherein the polymer is added to the suspension before it exits the outlet.

12. A method according to claim 1 in which the polymer is added in the form of an aqueous solution.

13. A method according to claim 1 in which the polymer is added in the form of particles.

14. A method according to claim 1 in which the mineral material is derived from mineral processing operations and is selected from the group consisting of red mud from a Bayer alumina process, tailings from the extraction of base metals, tailings from the extraction of precious metals, tailings from the extraction of iron, tailings from the extraction of nickel, coal tailings, mineral and oil sands and coal fines.

15. A method according to claim 1 in which the mineral material is hydrophilic in nature.

16. A method according to claim 1 in which the rehabilitation is further achieved by introducing into the deposition area plants, seedlings or seeds suitable for germination.

17. A method according to claim 1 in which the dewatered particulate mineral material is revegetated by hydroseeding.

18. The method according to claim 12 in which the polymer in the aqueous solution is in a concentration of 0.01% by weight.

19. The method according to claim 18 in which the polymer in the aqueous solution is in a concentration between 0.05% and 5% by weight.

20. The method according to claim 1 , wherein at least 80% of the polymer is water-soluble.

21. The method according to claim 1 , wherein aqueous liquor is released during step (i) and said aqueous liquor is substantially free of contaminants, and wherein said aqueous liquor is recycled.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 21, 2012
From: CIBA CORPORATION
To: BASF SE
Reel/Frame 028823/0704 →
CONDITIONAL ASSIGNMENT Recorded Sep 25, 2009
From: CIBA HOLDING INC.
To: CIBA CORPORATION
Reel/Frame 023284/0726 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 17, 2009
From: DYMOND, BRIAN; BELLWOOD, JOHN GERARD
To: CIBA HOLDING INC.
Reel/Frame 022275/0508 →