IP Library Granted Patent US 8,801,875
Granted Patent B2
US 8,801,875 · App. 12/336,120 · Granted Aug 12, 2014

Radiopaque alloy and medical device made of this alloy

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,801,875
App. No.
12/336,120
Granted
Aug 12, 2014
Kind
B2
Abstract

A radiopaque alloy based on titanium nickelide and having shape memory and superelastic properties includes, according to one embodiment, at least one radiopaque alloying element selected from among gold, platinum, and palladium at a concentration of from about 10 at. % to about 20 at. %, and at least one additional alloying element selected from among aluminum, chromium, cobalt, iron, and zirconium, where the additional alloying element has a concentration of from about 0.5 at. % to about 4 at. %. The alloy includes titanium at a concentration of from about 48 at. % to about 52 at. %, and the balance of the alloy is nickel. The radiopaque alloy preferably exhibits superelastic behavior suitable for medical device applications in the human body.

Claims (25)

1. A radiopaque alloy having shape memory and superelastic properties, consisting of:

titanium at a concentration of from about 48 to about 52 atomic percent;

at a concentration of from about 10 to about 35 atomic percent;

at least one additional alloying element selected from the group consisting of iron and cobalt at a concentration of from about 0.5 to about 8 atomic percent;

at least one further alloying element selected from the group consisting of aluminum, chromium, and zirconium at a concentration of from about 0.5 to about 4 atomic percent; and

nickel and inevitable impurities as a balance.

2. The alloy of claim 1 , wherein the nickel has a concentration of from about 29 at. % to about 52 at. %.

3. The alloy of claim 1 , wherein the alloy comprises:

gold at a concentration of about 20 at. %;

iron at a concentration of about 0.5 at. %; and

zirconium at a concentration of about 1 at. %.

4. The alloy of claim 1 , wherein the alloy comprises:

gold at a concentration of about 10 at. %;

iron at a concentration of about 1.2 at. %; and

zirconium at a concentration of about 1 at. %.

5. The alloy of claim 1 , wherein the alloy comprises:

gold at a concentration of about 15 at. %; and

aluminum at a concentration of about 1.2 at. %.

6. The alloy of claim 1 , wherein the alloy comprises:

gold at a concentration of about 15 at. %; and

chromium at a concentration of about 1 at. %.

7. The alloy of claim 1 , wherein the recoverable strain is at least about 5%.

8. The alloy of claim 1 , wherein the alloy is superelastic and has an austenite finish temperature at or below 37° C.

9. A medical device comprising at least one component comprising the radiopaque alloy of claim 1 .

10. The medical device of claim 9 , wherein the component comprises at least one of a wire and a cannula made of the radiopaque alloy.

Assignments (4)
SECURITY INTEREST Recorded Feb 28, 2024
From: COOK MEDICAL TECHNOLOGIES LLC
To: WILMINGTON TRUST, NATIONAL ASSOCIATION, AS COLLATERAL AGENT
Reel/Frame 066700/0277 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 3, 2017
From: LITHOTECH MEDICAL LTD.
To: NORDSON CORPORATION
Reel/Frame 044029/0714 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 22, 2014
From: COOK INCORPORATED
To: COOK MEDICAL TECHNOLOGIES LLC
Reel/Frame 032951/0405 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 4, 2009
From: DIAMANT, VALERY; KOREN, DAN; LOTKOV, ALEXANDER I.; SIVOKHA, VLADIMIR P.; MEYSNER, LIYDMILA L.; GRISHKOV, VIKTOR N.; VORONIN, VLADIMIR P.
To: COOK INCORPORATED; LITHOTECH MEDICAL LTD.
Reel/Frame 022344/0390 →