IP Library Granted Patent US 8,171,638
Granted Patent B2
US 8,171,638 · App. 12/341,267 · Granted May 8, 2012

Process for providing improved electrical properties on a roll for use in electrophotography

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,171,638
App. No.
12/341,267
Granted
May 8, 2012
Kind
B2
Abstract

A method and system for producing rolls for electrophotography are provided. The rolls can be rotated and shifted laterally during an oxidative baking process to produce finished rolls having improved electrical and printing characteristics. The oxidation of the rolls may be controlled to provide a corresponding increase in surface electrical resistance to within plus or minus 25 microns of a selected roll thickness.

Claims (35)

1. A method of oxidatively baking a roll in a heated fluid flow for use in electrophotography, comprising:

supporting said roll in a first position on a tray, wherein said roll is formed from a material that is capable of oxidation and an increase in electrical surface resistance;

altering the angle of the tray with respect to horizontal; and

moving said roll to a second position on the tray in the presence of said heated fluid and oxidizing and increasing the roll's electrical surface resistance;

wherein said roll has a shaft in which a distance between the first position and the second position being greater than about 0.25 of the circumference of said shaft.

2. The method of claim 1 wherein said roll oxidation and increase in electrical surface resistance is configured to occur for a selected thickness, and said oxidation and increase in electrical resistance occurs within plus or minus 25 microns of said selected thickness.

3. The method of claim 1 wherein said roll oxidation and increase in electrical surface resistance is configured to occur for a selected thickness, and said oxidation and increase in electrical resistance occurs within plus or minus 15 microns of said selected thickness.

4. The method of claim 1 wherein the roll rotates at least 90 degrees between the first position and the second position.

5. The method of claim 1 further comprising baking the roll at greater than 80° C. for greater than one hour.

6. The method of claim 1 wherein the roll is comprised of a polydiene polymer.

7. The method of claim 1 wherein the roll is comprised of a copolymer containing a polydiene component.

8. The method of claim 1 further comprising passing said heated fluid across the tray at a selected direction and velocity.

9. The method of claim 1 wherein said tray includes slots, and further comprising supporting the roll by contacting opposing ends of the roll's shaft to said slots in the tray without fixed attachment.

10. The method of claim 9 wherein the rolling step occurs in an oven at elevated temperature.

11. The method of claim 1 comprising altering the angle of the tray with respect to horizontal a second time to move the roll back to the first position.

12. The method of claim 1 wherein a plurality of rolls are supported on said tray and altering the angle of said tray results in rolling said plurality of rolls.

13. A method of improving the surface electrical resistance of a roll during an oxidative baking process, the method comprising;

positioning said roll on a tray;

passing a heated fluid across said roll, wherein said roll is formed from a material that is capable of oxidation and an increase in electrical surface resistance;

shifting the position of a roll's axis on the tray;

rotating said roll about its axis; and

oxidizing and increasing the roll's electrical surface resistance;

wherein said roll has a shaft in which a distance of the position shifting of the roll's axis being greater than about 0.25 of the circumference of said shaft.

14. The method of claim 13 wherein said roll oxidation and increase in electrical surface resistance is configured to occur for a selected thickness, and said oxidation and increase in electrical resistance occurs within plus or minus 25 microns of said selected thickness.

15. The method of claim 13 wherein said roll oxidation and increase in electrical surface resistance is configured to occur for a selected thickness, and said oxidation and increase in electrical resistance occurs within plus or minus 15 microns of said selected thickness.

16. The method of claim 13 further comprising supporting two ends of said shaft of the roll on the tray without fixed attachment.

17. The method of claim 13 wherein the roll is comprised of a polydiene polymer.

18. The method of claim 13 wherein the roll is comprised of a copolymer containing a polydiene component.

19. The method of claim 13 wherein shifting and rotating are performed simultaneously.

20. A method of oxidatively baking a roll in a heated fluid flow for use in electrophotography comprising:

supporting said roll in a first position on a tray, wherein said roll is formed from a polydiene polymer that is capable of oxidation and an increase in electrical surface resistance;

altering the angle of the tray with respect to horizontal; and

moving said roll to a second position on the tray in the presence of said heated fluid and oxidizing and increasing the roll's electrical surface resistance,

wherein said roll oxidation and increase in electrical surface resistance is configured to occur for a selected thickness, and said oxidation and increase in electrical resistance occurs within plus or minus 25 microns of said selected thickness, and

wherein said roll has a shaft in which a distance between the first position and the second position being greater than about 0.25 of the circumference of said shaft.

Assignments (4)
RELEASE OF SECURITY INTEREST Recorded Jan 18, 2024
From: CHINA CITIC BANK CORPORATION LIMITED, GUANGZHOU BRANCH, AS COLLATERAL AGENT
To: LEXMARK INTERNATIONAL, INC.
Reel/Frame 066345/0026 →
CORRECTIVE ASSIGNMENT TO CORRECT THE INCORRECT U.S. PATENT NUMBER PREVIOUSLY RECORDED AT REEL: 046989 FRAME: 0396. ASSIGNOR(S) HEREBY CONFIRMS THE PATENT SECURITY AGREEMENT. Recorded Oct 24, 2018
From: LEXMARK INTERNATIONAL, INC.
To: CHINA CITIC BANK CORPORATION LIMITED, GUANGZHOU BRANCH, AS COLLATERAL AGENT
Reel/Frame 047760/0795 →
PATENT SECURITY AGREEMENT Recorded Aug 30, 2018
From: LEXMARK INTERNATIONAL, INC.
To: CHINA CITIC BANK CORPORATION LIMITED, GUANGZHOU BRANCH, AS COLLATERAL AGENT
Reel/Frame 046989/0396 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 22, 2008
From: KRAL, DONALD THOMAS; SEARLS, SCOTT ALAN
To: LEXMARK INTERNATIONAL, INC.
Reel/Frame 022016/0313 →