IP Library Granted Patent US 8,176,859
Granted Patent B2
US 8,176,859 · App. 12/357,823 · Granted May 15, 2012

Refractory brick and tapered mortar joint

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,176,859
App. No.
12/357,823
Granted
May 15, 2012
Kind
B2
Abstract

A refractory brick and mortar joint comprise a cold face of the refractory brick; a hot face of the refractory brick opposite the cold face, wherein the hot face is shorter in length than the cold face; and at least one tapered mortar joint extending from the hot face to the cold face, wherein the at least one tapered mortar joint is thicker at the hot face of the refractory brick than at the cold face of the refractory brick. A refractory brick comprises a cold face; a hot face opposite the cold face, wherein the hot face is shorter in length than the cold face; and at least one surface extending from the cold face to the hot face, wherein the at least one surface is angled to accommodate the difference in length between the cold face and the hot face.

Claims (14)

1. A refractory brick and mortar joint, comprising:

a cold face of the refractory brick;

a hot face of the refractory brick opposite the cold face, wherein the hot face is shorter in length than the cold face; and

at least one tapered mortar joint extending from the hot face to the cold face, wherein the at least one tapered mortar joint is thicker at the hot face of the refractory brick than at the cold face of the refractory brick, wherein the at least one tapered mortar joint is uniform in thickness near the cold face, and tapered near the hot face.

2. The refractory brick and mortar joint of claim 1 , wherein the at least one tapered mortar joint has a taper angle between approximately 0 degrees and approximately 20 degrees.

3. A method of making a lining for a gasifier chamber, comprising:

placing a plurality of refractory bricks about a perimeter of a gasifier, each of the plurality of refractory bricks comprising a cold face, and a hot face opposite the cold face, the hot face being shorter in length than the cold face; and

interspersing a plurality of tapered mortar joints between the plurality of refractory bricks such that each tapered mortar joint is thicker at the hot face of a refractory brick than at the cold face of a refractory brick, wherein each tapered mortar joint of the plurality of tapered mortar joints is uniform in thickness near the cold face, and tapered near the hot face.

4. The method of claim 3 , wherein each tapered mortar joint of the plurality of tapered mortar joints has a taper angle between approximately 0 degrees and approximately 20 degrees.

5. A refractory brick, comprising:

a cold face;

a hot face opposite the cold face, wherein the hot face is shorter in length than the cold face; and

at least one surface extending from the cold face to the hot face, wherein the at least one surface is angled to accommodate the difference in length between the cold face and the hot face, wherein the at least one surface is perpendicular to the cold face, and angled with respect to the hot face.

6. The refractory brick of claim 5 , wherein the angle between the at least one surface and the hot face is between approximately 90 degrees and approximately 110 degrees.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 22, 2019
From: GENERAL ELECTRIC COMPANY
To: AIR PRODUCTS AND CHEMICALS, INC.
Reel/Frame 050786/0768 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 23, 2009
From: GUO, CLIFF YI; CHEN, WEI; TALYA, SHASHISHEKARA SITHARAMARAO
To: GENERAL ELECTRIC COMPANY
Reel/Frame 022146/0939 →