Method for stamping thermally activatable adhesive materials which are not tacky at room temperature

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,062,458
App. No.
12/374,805
Granted
Nov 22, 2011
Kind
B2
Abstract

Method for producing diecuts from heat-activatable adhesive films which comprises applying a layer of heat-activatable adhesive material to a carrier material having a glass transition temperature at least 20° C. lower that that of the adhesive, laminating the heat-activatable layer onto a release liner at a temperature between the glass transition temperature of the release liner and heat activatable adhesive and then diecutting the heat-activatable adhesive layer on the release liner.

Claims (8)

1. A method of producing diecuts from heat-activatable adhesive films, which comprises

a. coating a heat-activatable adhesive initially onto a first carrier material,

b. laminating the heat-activatable adhesive layer onto a release liner having a glass transition temperature at least 20° C. lower than the glass transition temperature of the heat-activatable adhesive, at a temperature between the glass transition temperature of the release liner and the glass transition temperature of the heat-activatable adhesive, the release liner having at least one polyolefin-based surface, and the polyolefinic surface being nontacky at room temperature and having pressure-sensitive adhesive properties at the temperature at which said lamination is carried out,

c. and diecutting the heat-activatable adhesive layer on the release liner.

2. The method of claim 1 , wherein said release liner has a glass transition temperature of at least 30° C. lower than the glass temperature of the heat-activatable pressure-sensitive adhesive.

3. The method of claim 1 , wherein the release liner is an at least two-layer film.

4. The method of claim 3 , wherein the release liner is a coextruded film comprising a polyolefin layer and a layer of polyester, polymethyl methacrylate, polyimide, polyethylene naphthalate, polyurethane or polyamide.

5. The method of claim 3 , wherein the release liner is a film comprising a polyolefin layer and a layer of polyethylene or polypropylene.

Assignments (2)
CHANGE OF NAME Recorded Oct 7, 2010
From: TESA AG
To: TESA SE
Reel/Frame 025107/0973 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 19, 2009
From: HUSEMANN, MARC; HANNEMANN, FRANK
To: TESA AG
Reel/Frame 022281/0256 →