IP Library Granted Patent US 8,215,371
Granted Patent B2
US 8,215,371 · App. 12/417,740 · Granted Jul 10, 2012

Digital manufacturing with amorphous metallic alloys

Assignee: Stratasys, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,215,371
App. No.
12/417,740
Granted
Jul 10, 2012
Kind
B2
Abstract

A method for building a three-dimensional object in a layer-by-layer manner, the method comprising heating a build chamber of a digital manufacturing system, feeding a solid feedstock of a modeling material comprising an amorphous metallic alloy to a liquefier assembly of the digital manufacturing system, heating the modeling material of the solid feedstock in the liquefier assembly to an extrudable state, and depositing the heated modeling material within the heated build chamber in a predetermined pattern to form the three-dimensional object.

Claims (26)

1. A method for building a three-dimensional object in a layer-by-layer manner with an extrusion-based digital manufacturing system having a build chamber, the method comprising:

providing a supply source to the extrusion-based digital manufacturing system at a remote location from the build chamber, the supply source comprising a modeling material, wherein the modeling material comprises an amorphous metallic alloy having a melting temperature, a glass transition temperature less than about 450° C., a creep relaxation temperature, and a solidification temperature, wherein the difference between the glass transition temperature and the melting temperature is at least about 20° C., and wherein the modeling material has a wire geometry formed from a reheated and shaped solid material of the amorphous metallic alloy;

heating the build chamber of the extrusion-based digital manufacturing system to one or more temperatures within a window ranging from the solidification temperature and the creep relaxation temperature of the modeling material;

feeding the modeling material from the supply source disposed at the remote location from the build chamber, through a portion of the extrusion-based digital manufacturing system, and to a liquefier assembly retained by the extrusion-based digital manufacturing system;

heating the modeling material of the solid feedstock in the liquefier assembly to an extrudable state; and

depositing the heated modeling material within the heated build chamber in a predetermined pattern to form the three-dimensional object.

2. The method of claim 1 , wherein the liquefier assembly comprises a liquefier tube and a coating on an inner surface of the liquefier tube that is configured to reduce alloying of the amorphous metallic alloy of the modeling material to the inner surface of the liquefier tube.

3. The method of claim 1 , wherein the glass transition temperature of the amorphous metallic alloy is less than about 250° C.

4. The method of claim 1 , wherein the difference between the glass transition temperature and the melting temperature of the modeling material is at least about 50° C.

5. The method of claim 1 , wherein the amorphous metallic alloy comprises cerium, copper, aluminum, and niobium.

6. The method of claim 1 , wherein the amorphous metallic alloy comprises an alloy having a chemical formula of Ce 68 Cu 20 Al 10 Nb 2 .

7. The method of claim 1 , wherein the wire geometry has an average diameter ranging from about 0.508 millimeters to about 2.54 millimeters.

8. A method for building a three-dimensional object in a layer-by-layer manner with an extrusion-based digital manufacturing system having a build chamber, the method comprising:

providing a first container to the extrusion-based digital manufacturing system at a remote location from the build chamber, wherein the first container has a modeling material that comprises an amorphous metallic alloy and has a melting temperature, a glass transition temperature less than about 450° C., a creep relaxation temperature, and a solidification temperature, wherein the difference between the glass transition temperature and the melting temperature is at least about 20° C. and wherein the modeling material has a wire geometry formed from a reheated and shaped solid material of the amorphous metallic alloy;

providing a second container to the extrusion-based digital manufacturing system, wherein the second container has a filament of support material that comprises a thermoplastic material and has a creep relaxation temperature and a solidification temperature, and wherein a difference between the creep relaxation temperatures of the modeling material and the support material is less than about 30° C.;

heating the build chamber of the extrusion-based digital manufacturing system to one or more temperatures within a window ranging from the solidification temperature and the creep relaxation temperature of the modeling material;

feeding the modeling material from the first container disposed at the remote location from the build chamber, through a portion of the extrusion-based digital manufacturing system, and to an extrusion head retained by the extrusion-based digital manufacturing system;

plastic-metal extruding the modeling material from the extrusion head in a first predetermined pattern within the heated build chamber to form the three-dimensional object;

feeding the support material from the second container to the extrusion head; and

thermoplastic extruding the support material from the extrusion head in a second predetermined pattern within the heated build chamber to form a support structure for the three-dimensional object.

9. The method of claim 8 , wherein the support material further comprises a fluxing material.

10. The method of claim 8 , wherein the difference between the creep relaxation temperatures of the modeling material and the support material is less than about 20° C.

11. The method of claim 8 , wherein the wire geometry of the modeling material has an average diameter ranging from about 0.508 millimeters to about 2.54 millimeters.

12. The method of claim 11 , wherein the filament of the support material has an average diameter ranging from about 1.143 millimeters to about 2.54 millimeters.

13. The method of claim 8 , wherein the amorphous metallic alloy comprises cerium, copper, aluminum, and niobium.

14. The method of claim 8 , wherein the amorphous metallic alloy comprises an alloy having a chemical formula of Ce 68 Cu 20 Al 10 Nb 2 .

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 3, 2009
From: BATCHELDER, JOHN SAMUEL
To: STRATASYS, INC.
Reel/Frame 022499/0398 →
Continuity (2)
Provisional Application 61124646 · Apr 18, 2008
Related Publication 20090263582A1 · Oct 22, 2009