Phosphor and method for manufacturing the same, and light-emitting device and display device using phosphor
A phosphor includes (Sr 1−x , Ba x ) 3 SiO 5 with 1>x≧0.1 as a base material and europium (Eu) as an activator. The emission center wavelength of the phosphor is controlled to be 600 nm or more on the basis of the composition ratio of Sr, Ba, and Eu.
1. A method for manufacturing a phosphor including (Sr 1−x , Ba x ) 3 SiO 5 as a base material and europium (Eu) as an activator, comprising:
preparing a mixture of compounds respectively including Sr, Ba, Si, and Eu such that a molar ratio of Sr, Ba, and Si is Sr:Ba:Si=3(1−x):3x:1 where 0.5≧x≧0.25, and a ratio of the number of moles of Eu to a total number of moles of Sr, Ba, and Eu is 0.06 or more and 0.08 or less; and
firing the mixture at 1600° C. or more and 1700° C. or less in an inert gas atmosphere containing 4% or less of hydrogen on a volume basis,
wherein a peak emission wavelength of the phosphor is 600 nm or more based on a composition ratio of Sr, Ba, and Eu.
2. The method for manufacturing the phosphor according to claim 1 that emits fluorescence when excited with blue light.