IP Library Granted Patent US 8,287,464
Granted Patent B2
US 8,287,464 · App. 12/516,303 · Granted Oct 16, 2012

Metal needle usable in echo imaging

Assignee: Nipro Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,287,464
App. No.
12/516,303
Granted
Oct 16, 2012
Kind
B2
Abstract

A metal needle is obtained by being dipped in a liquid selected from the group consisting of a strong acid solution of a metal, acetic acid, and butyl acetate, and then dried. Preferably, the strong acid solution of a metal to be used in the dipping treatment may be a nitric acid solution of a metal selected from the group consisting of a transition element, a lanthanoid, and an actinoid, for example, a nitric acid solution of a metal selected from the group consisting of palladium, gadolinium, germanium, beryllium, strontium, scandium, and samarium. The metal needle is a metal needle for insertion into the body that can be reliably imaged even when a general-purpose ultrasound imaging system is used, and thus is useful in confirming insertion of the needle into a blood vessel and arrival of the needle at an organ, and confirming the position of the needle when it is broken.

Claims (11)

1. A method of obtaining a metal needle that is visible in echo imaging, the method comprising the steps of: dipping the metal needle in a strong acid solution of a metal, and drying the needle, wherein the strong acid solution of a metal is a nitric acid solution of a metal selected from the group consisting of a transition element, a lanthanoid, and an actinoid.

2. The method of claim 1 , wherein the strong acid solution of a metal is a nitric acid solution of a metal selected from the group consisting of palladium, gadolinium, germanium, beryllium, strontium, scandium, and samarium.

3. The method of claim 2 , wherein the strong acid solution of a metal has a concentration of the metal of 980 to 1020 mg/L and a concentration of the strong acid of 0.08 to 1.1 mol/L.

4. The method of claim 2 , wherein the metal needle is for tissue collection.

5. The method of claim 2 , wherein the solution is a standard stock solution for atomic absorption spectrometry.

6. The method of claim 1 , wherein the strong acid solution of a metal has a concentration of the metal of 980 to 1020 mg/L and a concentration of the strong acid of 0.08 to 1.1 mol/L.

7. The method of claim 6 , wherein the metal needle is for tissue collection.

8. The method of claim 6 , wherein the solution is a standard stock solution for atomic absorption spectrometry.

9. The method of claim 1 , wherein the metal needle is for tissue collection.

10. The method of claim 9 , wherein the solution is a standard stock solution for atomic absorption spectrometry.

11. The method of claim 1 , wherein the solution is a standard stock solution for atomic absorption spectrometry.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 26, 2009
From: HIROTA, HIROSHI; IWASE, YOSHIHARU
To: NIPRO CORPORATION
Reel/Frame 022735/0021 →
Priority Claims (1)
JP 2007-093359 · Mar 30, 2007 · national
Continuity (1)
Related Publication 20100069789A1 · Mar 18, 2010