IP Library Granted Patent US 8,523,958
Granted Patent B2
US 8,523,958 · App. 12/526,569 · Granted Sep 3, 2013

Fabrication of lithium secondary battery

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,523,958
App. No.
12/526,569
Granted
Sep 3, 2013
Kind
B2
Abstract

A method of fabricating a lithium secondary battery, which improves charge-discharge characteristics, lifespan, and temperature characteristics of the battery and which includes interposing a separator between a positive electrode plate and a negative electrode plate, thus manufacturing an electrode assembly; housing the electrode assembly in a battery case, introducing an additive-containing electrolytic solution, and then sealing the battery case; subjecting the sealed battery case to pre-charging, and then removing gas generated by the pre-charging; subjecting the battery case to formation; and removing gas generated by the formation, wherein the additive is one or more selected from among LiF 2 BC 2 O 4 , 3,9-divinyl-2,4,8,10-tetraoxaspiro[5,5]undecane, LiB(C 2 O 4 ) 2 , poly(ethyleneglycol)borate and derivatives thereof, halogen-substituted carbonate, and vinyl silane, and the pre-charging is conducted in a range of 10% or less of a battery capacity.

Claims (14)

1. A method of fabricating a lithium secondary battery, comprising:

interposing a separator between a positive electrode plate and a negative electrode plate, thus manufacturing an electrode assembly;

housing the electrode assembly in a battery case, introducing an additive-containing electrolytic solution, and then sealing the battery case;

subjecting the sealed battery case to pre-charging, and then removing gas generated by the pre-charging;

subjecting the battery case to formation; and

removing gas generated by the formation,

wherein the additive is one or more selected from the group consisting of LiF 2 BC 2 O 4 , 3,9-divinyl-2,4,8,10-tetraoxaspiro[5,5]undecane, LiB(C 2 O 4 ) 2 , poly(ethyleneglycol)borate and vinyl silane, and

the pre-charging is conducted in a range of 10% or less of the lithium secondary battery capacity,

wherein the pre-charging is conducted under conditions of current of 0.1˜1 C and voltage of 3.6 to less than 4.4 V.

2. The method according to claim 1 , wherein:

the battery case is connected with a first as chamber and a second gas chamber through respective connection paths,

the removing gas generated by the pre-charging is conducted by exhausting the gas into the first gas chamber, thermally compressing and sealing the connection path between the first gas chamber and the battery case, and then eliminating the first gas chamber from the battery case, and

the removing gas generated by the formation is conducted by exhausting the gas into the second gas chamber, thermally compressing and sealing the connection path between the second gas chamber and the battery case, and then eliminating the second gas chamber from the battery case.

3. The method according to claim 1 , wherein the additive is used in an amount of 0.1˜10.0 wt % based on an amount of a final electrolytic solution.

Assignments (2)
CHANGE OF ADDRESS Recorded Nov 7, 2022
From: SK INNOVATION CO., LTD.
To: SK INNOVATION CO., LTD.
Reel/Frame 061895/0380 →
NUNC PRO TUNC ASSIGNMENT Recorded Nov 7, 2022
From: SK INNOVATION CO., LTD.
To: SK ON CO., LTD.
Reel/Frame 062034/0198 →