Rubber composition and vulcanized rubber product using the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,758,937
App. No.
12/530,044
Granted
Jul 20, 2010
Kind
B2
Abstract

Disclosed is a rubber composition excellent in oil resistance and weather resistance, while having excellent adhesion to a brass. Also disclosed is a vulcanized rubber product using such a rubber composition. Specifically disclosed is a rubber composition containing a rubber component (A), an inorganic filler (B), a plasticizer (C) and a process oil (D). The rubber component (A) contains 30-60% by mass of an acrylonitrile-butadiene rubber, 20-40% by mass of an ethylene-propylene-nonconjugated diene rubber, and 20-50% by mass of a styrene-butadiene rubber. The inorganic filler (B) is contained in the composition in an amount of 5-100 parts by mass per 100 parts by mass of the rubber component (A), and the mass ratio between the plasticizer (C) and the process oil (D) is from 15/85 to 75/25. Also specifically disclosed is a vulcanized rubber product obtained by vulcanizing such a rubber composition.

Claims (14)

1. A vulcanizing rubber product comprising: a rubber layer obtained by vulcanizing a rubber composition comprising a rubber component (A), an inorganic filler (B), a plasticizer (C), and a process oil (D); and a brass-plated reinforced layer adjoining to the rubber layer, wherein

the rubber component (A) contains 30 to 50 wt % of an acrylonitrile-butadiene rubber, 20 to 35 wt % of an ethylene-propylene-nonconjugated diene rubber, and 25 to 50 wt % of a styrene-butadiene rubber,

the inorganic filler (B) is clay,

the content of the inorganic filler (B) is 10 to 100 parts by weight with respect to 100 parts by weight of the rubber component (A), and

the weight ratio of the plasticizer (C) to the process oil (D) is 15/85 to 75/25.

2. The vulcanized rubber product of claim 1 which is a hose.

3. The vulcanized rubber product of claim 1 which is a hydraulic hose or a high-pressure hose.

4. A hose comprising an inner rubber layer, a brass-plated reinforced layer disposed so as to adjoin to a circumferential side of the inner rubber layer, and an outer rubber layer disposed so as to adjoin a circumferential side of the reinforced layer, wherein

at least the outer rubber layer is formed from a rubber composition comprising a rubber component (A), an inorganic filler (B), a plasticizer (C), and a process oil (D),

the rubber component (A) contains 30 to 50 wt % of an acrylonitrile-butadiene rubber, 20 to 35 wt % of an ethylene-propylene-nonconjugated diene rubber, and 25 to 50 wt % of a styrene-butadiene rubber,

the inorganic filler (B) is clay,

the content of the inorganic filler (B) is 10 to 100 parts by weight with respect to 100 parts by weight of the rubber component (A), and

the weight ratio of the plasticizer (C) to the process oil (D) is 15/85 to 75/25.

5. The vulcanized rubber product of claim 2 which is a hydraulic hose or a high-pressure hose.

Assignments (2)
CHANGE OF ADDRESS FOR ASSIGNEE Recorded Nov 18, 2023
From: THE YOKOHAMA RUBBER CO., LTD.
To: THE YOKOHAMA RUBBER CO., LTD.
Reel/Frame 065626/0740 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 4, 2009
From: GONG, PENG; OISHI, HIDEYUKI; SATO, AKIRA; TORII, NAOTO
To: THE YOKOHAMA RUBBER CO., LTD.
Reel/Frame 023197/0107 →