IP Library Granted Patent US 8,573,949
Granted Patent B2
US 8,573,949 · App. 12/571,358 · Granted Nov 5, 2013

Method and system for focused energy brazing

Inventors: Yan Cui (Greenville, SC); Srikanth Chandrudu Kottilingam (Simpsonville, SC); Gene Murphy (Pelzer, SC)
Assignee: General Electric Company
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,573,949
App. No.
12/571,358
Granted
Nov 5, 2013
Kind
B2
Abstract

A method and system that includes generation of an energy beam. The energy beam may be generated from a focused energy source. Additionally, the energy beam may be directed towards a pre-sintered preform. The pre-sintered preform may be made of a braze material and may seal a hole that may be located in a turbine component.

Claims (28)

1. A system, comprising:

a focused energy source configured to generate an energy beam; and

a brazing controller configured to control brazing of a pre-sintered preform via alteration of at least one performance characteristic of the focused energy source to adjust the energy beam for focused brazing of the pre-sintered preform.

2. The system of claim 1 , wherein the focused energy source comprises an electron beam welder configured to generate the energy beam as an electron energy beam.

3. The system of claim 2 , comprising a beam deflector, wherein the controller is configured to control the beam deflector to adjust a path of the energy beam.

4. The system of claim 3 , wherein the controller is configured to control the beam deflector to adjust a focal point of the energy beam.

5. The system of claim 4 , wherein the focal point is adjusted to be located at approximately 0.1 to 2 inches above the pre-sintered preform.

6. The system of claim 1 , wherein the least one performance characteristic of the focused energy source comprises an energy intensity of the energy beam.

7. The system of claim 1 , wherein the focused energy source comprises a laser welder configured to generate a laser energy beam.

8. The system of claim 1 , comprising a sensor configured to detect parameters relating to a brazing process performed via the focused energy source.

9. The system of claim 8 , wherein the detected parameters include an ambient temperature, a heat level of the energy beam, or movement of the energy beam.

10. The system of claim 8 , wherein the sensor is configured to transmit the detected parameters to the controller to adjust the at least one performance characteristic of the focused energy source.

11. A system, comprising:

a turbine component comprising a superalloy; and

a pre-sintered preform (PSP) braze material disposed on a portion of the turbine component and bonded to the turbine component via brazing, wherein the portion of the turbine component not bonded to the PSP braze material is materially unchanged due to the brazing.

12. The system of claim 11 , wherein the turbine component comprises a turbine bucket or a turbine nozzle.

13. The system of claim 11 , wherein the PSP braze material is disposed in a hole of the turbine component.

14. The system of claim 11 , wherein the PSP braze materials are independently heated and solidified via a focused energy beam.

15. The system of claim 11 , comprising:

a focused energy source configured to generate an energy beam for focused brazing of the turbine component and first and second braze materials comprising the PSP braze material; and

a controller configured to adjust at least one characteristic of the energy beam, wherein the at least one characteristic comprises a focal point of the energy beam or an intensity of the energy beam.

16. The system of claim 15 , wherein the focused energy source comprises an electron beam welder or a laser beam welder.

17. A method, comprising:

generating an energy beam from a focused energy source; and

directing the energy beam toward a pre-sintered preform of a braze material to seal a hole in a turbine component.

18. The method of claim 17 , comprising moving the energy beam in a pattern via one or more beam deflectors.

19. The method of claim 17 , comprising raising the temperature of the pre-sintered preform between approximately 200 and 500 degrees Fahrenheit per minute.

20. The method of claim 17 , comprising heating the pre-sintered preform to approximately between 2000 and 2275 degrees Fahrenheit for approximately between one and five minutes.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 1, 2009
From: CUI, YAN; KOTTILINGAM, SRIKANTH CHANDRUDU; MURPHY, GENE
To: GENERAL ELECTRIC COMPANY
Reel/Frame 023311/0336 →
Continuity (1)
Related Publication 20110076151A1 · Mar 31, 2011