IP Library Granted Patent US 7,939,175
Granted Patent B2
US 7,939,175 · App. 12/609,723 · Granted May 10, 2011

Non-halogenated rubber compounds for use in conveyor belts

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,939,175
App. No.
12/609,723
Granted
May 10, 2011
Kind
B2
Abstract

A non-halogenated rubber compound is provided for use in conveyor belts, particularly those used in underground mining. The non-halogenated rubber compound is fire-resistant in accordance with MSHA standards and produces acceptable levels of toxicity and smoke upon burning. Such non-halogenated rubber compound includes a blend of rubbery polymers in combination with aluminum trihydrate, which is a fire retardant, and optionally a phosphate plasticizer, which can provide the rubber compound with a more desirable workability. The blend of rubbery polymers is composed of natural rubber and butadiene rubber, and optionally styrene-butadiene rubber, such blend being present in a total amount of 100 phr. In one embodiment, the aluminum trihydrate is present in an amount of about 30 phr to about 150 phr. In another embodiment, the phosphate plasticizer is present in an amount of about 10 phr to about 60 phr.

Claims (5)

1. A fire-resistant conveyor belt comprising:

a first and second outer cover layer situated on the outer opposing surfaces of the conveyor belt, the first and second outer layers defining a non-halogenated rubber compound consisting of aluminum trihydrate, about 10 phr to about 60 phr of a phosphate plasticizer, and a blend of rubber polymers present in a total amount of 100 phr, the blend of rubbery polymers consisting of natural rubber and polybutadiene rubber; wherein the natural rubber is present in the blend at a level which is within the range of about 30 phr to about 70 phr, and wherein the blend of rubbery polymers is void of nitrile-group containing polymers, and

at least one reinforcement layer situated between the first cover layer and the second cover layer, wherein the conveyor belt is fire-resistant, and wherein the at least one reinforcement layer includes outer first and second skim layers on opposing surfaces of the reinforcements layers, the outer first and second skim layers being comprised of the non-halogenated rubber.

2. The fire-resistant conveyor belt of claim 1 wherein the blend of rubbery polymers is void of red phosphorous.

3. The fire-resistant conveyor belt of claim 1 wherein the aluminum trihydrate is present at a level which is within the range of about 30 phr to about 150 phr.

Assignments (3)
CHANGE OF NAME Recorded Feb 10, 2025
From: CONTITECH USA, INC.
To: CONTITECH USA, LLC
Reel/Frame 070615/0527 →
CHANGE OF NAME Recorded Aug 30, 2017
From: VEYANCE TECHNOLOGIES, INC
To: CONTITECH USA, INC.
Reel/Frame 043715/0469 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 24, 2011
From: ALEXANDER, KENNETH MICHAEL; MAGUIRE, DAVID JOSEPH
To: VEYANCE TECHNOLOGIES, INC.
Reel/Frame 026011/0573 →