Method of forming protrusions on the inner surface of a tube

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,302,307
App. No.
12/622,487
Granted
Nov 6, 2012
Kind
B2
Abstract

A method of forming a plurality of protrusions on the inner surface of a tube to reduce tube side resistance and improve overall heat transfer performance. The method includes cutting through ridges on the inner surface of the tube to create ridge layers and lifting the ridge layers to form the protrusions. In this way, the protrusions are formed without removal of metal from the inner surface of the tube, thereby eliminating debris which can damage the equipment in which the tubes are used.

Claims (22)

1. A method of manufacturing a tube having a surface, a longitudinal axis, ridges extending along the tube surface, and a plurality of primary grooves each extending along the tube surface between adjacent ridges, the method comprising:

a. cutting through at least one ridge to a cutting depth and at an angle relative to the longitudinal axis to form ridge layers; and

b. lifting the ridge layers upwardly relative to the surface of the tube to form (i) a plurality of protrusions along the at least one ridge and (ii) secondary grooves extending between and connecting adjacent primary grooves between which the at least one ridge extends,

wherein at least some of the plurality of protrusions project from the surface in a direction that is not substantially perpendicular to the longitudinal axis.

2. The method of claim 1 , wherein the plurality of protrusions are formed on the inner surface of the tube.

3. The method of claim 1 , wherein each of the plurality of protrusions has a height that is a value no more than three times the cutting depth.

4. The method of claim 2 , wherein the tube has an inside diameter and each of the plurality of protrusions has a height, wherein the ratio of each protrusion height to tube inside diameter is between approximately 0.002 and 0.5.

5. The method of claim 1 , wherein other of the plurality of protrusions extend from the surface in a direction substantially perpendicular to the longitudinal axis.

6. The method of claim 1 , wherein the secondary grooves extend at an angle between approximately 80° and 100° relative to the longitudinal axis of the tube.

7. The method of claim 1 , wherein the at least one ridge is cut through at an angle between approximately 20° and 50° relative to the longitudinal axis of the tube.

8. The method of claim 1 , wherein the at least one ridge has a ridge height and the cutting depth approximately equals the ridge height.

9. The method of claim 1 , wherein the at least one ridge has a ridge height and the cutting depth does not equal the ridge height.

10. The method of claim 1 , wherein at least some of the plurality of protrusions comprise a sloped top surface.

11. The method of claim 1 , wherein at least some of the plurality of protrusions comprise a pointed tip.

12. A method of manufacturing a tube having a surface and a longitudinal axis comprising using a tool having at least one tool tip (i) to cut with the at least one tool tip through at least one ridge formed along the surface of the tube to a cutting depth and at an angle relative to the longitudinal axis to form ridge layers and (ii) to lift with the at least one tool tip the ridge layers upwardly relative to the surface of the tube to form a plurality of protrusions along the at least one ridge and secondary grooves extending between and connecting adjacent primary grooves between which the at least one ridge extends, wherein at least some of the plurality of protrusions project from the surface in a direction that is not substantially perpendicular to the longitudinal axis.

13. The method of claim 12 , wherein the tool tip comprises a cutting edge to cut through the at least one ridge and a lifting edge to lift the ridge layers.

14. The method of claim 12 , wherein the plurality of protrusions are formed on the inner surface of the tube.

15. The method of claim 12 , wherein other of the plurality of protrusions extend from the surface in a direction substantially perpendicular to the longitudinal axis.

16. The method of claim 12 , wherein the at least one ridge has a ridge height and the cutting depth approximately equals the ridge height.

17. The method of claim 12 , wherein the at least one ridge has a ridge height and the cutting depth does not equal the ridge height.

18. The method of claim 12 , wherein at least some of the plurality of protrusions comprise a sloped top surface.

19. The method of claim 12 , wherein at least some of the plurality of protrusions comprise a pointed tip.

Assignments (6)
TERMINATION AND RELEASE Recorded May 23, 2013
From: U.S. BANK NATIONAL ASSOCIATION
To: WOLVERINE TUBE, INC.; TUBE FORMING, L.P.; WT HOLDING COMPANY INC.; WOLVERINE JOINING TECHNOLOGIES, LLC
Reel/Frame 030487/0555 →
PATENT ASSIGNMENT AGREEMENT Recorded May 7, 2013
From: WOLVERINE TUBE, INC.
To: WIELAND-WERKE AG
Reel/Frame 030361/0918 →
RELEASE OF SECURITY INTEREST Recorded May 1, 2013
From: JPMORGAN CHASE BANK, N.A.
To: WOLVERINE TUBE, INC.
Reel/Frame 030326/0221 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 28, 2011
From: THORS, PETUR; ZOUBKOV, NIKOLAI
To: WOLVERINE TUBE, INC.
Reel/Frame 027453/0228 →
SECURITY AGREEMENT Recorded Nov 15, 2011
From: WOLVERINE TUBE, INC.; WOLVERINE JOINING TECHNOLOGIES, LLC
To: JPMORGAN CHASE BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 027232/0423 →
SECURITY AGREEMENT Recorded Jul 8, 2011
From: WOLVERINE TUBE, INC.
To: U.S. BANK NATIONAL ASSOCIATION
Reel/Frame 026562/0557 →