IP Library Granted Patent US 8,273,799
Granted Patent B2
US 8,273,799 · App. 12/634,708 · Granted Sep 25, 2012

Amination of vinyl aromatic polymers with tertiary amines

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,273,799
App. No.
12/634,708
Granted
Sep 25, 2012
Kind
B2
Abstract

The invention generally relates to amination reactions and amination reaction products, and particularly to methods for aminating vinyl aromatic polymers utilizing tertiary amines. In one embodiment, the invention includes conducting an amination reaction by combining a tertiary amine and a vinyl aromatic polymer comprising benzyl chloride groups to form a reaction mixture and maintaining the pH of the reaction mixture within a designated range. In another embodiment, the invention includes an aminated vinyl aromatic polymer. In yet another embodiment, the invention includes an ion exchange resin including quaternary ammonium functionality. The invention is useful in preparing ion exchange resins suitable for a variety of applications such as the removal of perchlorate ions from water sources and recovery of gold cyanide from mining leach solutions.

Claims (26)

1. A method of conducting an amination reaction by:

i) combining a tertiary amine and a vinyl aromatic polymer comprising benzyl chloride groups in a ratio of less than 1.5 mole of tertiary amine per mole of benzyl chloride group of the vinyl aromatic polymer within an alcohol-based solvent to form a reaction mixture, wherein the tertiary amine is represented by the formula:

wherein R 1 , R 2 and R 3 are each independently selected from: alkyl and alkoxy groups; with the proviso that the total number of carbon atoms for R 1 , R 2 and R 3 is at least 7;

ii) conducting an amination reaction for a reaction time period of at least 2 hours; and

iii) maintaining the reaction mixture at a temperature of at least 50° C. and a pH of at least 7 for at least half of the reaction time period by adding a base selected from at least one of: sodium hydroxide, sodium carbonate, calcium hydroxide, calcium oxide and potassium hydroxide.

2. The method of claim 1 wherein the reaction mixture is maintained within a pH range of from 8.5 to 11.5 for at least half of the reaction time period by the addition of a base to the reaction mixture, wherein the base is selected from at least one of: sodium hydroxide, sodium carbonate, calcium hydroxide, calcium oxide and potassium hydroxide.

3. The method of claim 1 wherein a base is repeatedly added to the reaction mixture during the reaction time period and wherein the base is selected from at least one of: sodium hydroxide, sodium carbonate, calcium hydroxide, calcium oxide and potassium hydroxide.

4. The method of claim 1 wherein the alcohol-based solvent comprises methanol.

5. The method of claim 1 wherein the tertiary amine is selected from at least one of: tripropyl amine, tributyl amine, tripentyl amine and trihexyl amine.

6. The method of claim 1 wherein the vinyl aromatic polymer comprising benzyl chloride groups comprises repeating units represented by the formula:

wherein the benzyl chloride group is located at the meta, ortho or para position.

7. The method of claim 1 wherein a reaction product of the amination reaction comprises a vinyl aromatic polymer comprising repeating units represented by the formula:

wherein R 1 , R 2 and R 3 are each independently selected from: alkyl and alkoxy groups; with the proviso that the total number of carbon atoms for R 1 , R 2 and R 3 is at least 7.

8. The method of claim 1 wherein a reaction product of the amination reaction comprises a vinyl aromatic polymer comprising repeating units represented by the formula:

wherein R 1 , R 2 and R 3 are each independently selected from alkyl groups comprising from 1 to 8 carbon atoms with the proviso that the total number of carbon atoms for R 1 , R 2 and R 3 is at least 8.

9. The method of claim 1 wherein the reaction time period is at least 6 hours.

10. The method of claim 1 wherein the alcohol-based solvent comprises at least: 30 weight percent methanol, 20 weight percent methylal and 10 weight percent water.

11. The method of claim 1 wherein the step of combining a tertiary amine and a vinyl aromatic polymer further comprises combining the reactants in a ratio of less than or equal to one mole of tertiary amine per mole of benzyl chloride group of the vinyl aromatic polymer.

12. A method of claim 1 comprising:

i) a tertiary amine represented by the formula:

wherein R 1 , R 2 and R 3 are each independently selected from: alkyl groups having from 1 to 8 carbon atoms and alkyoxy groups having from 2 to 8 carbon atoms, with the proviso that the total number of carbon atoms for R 1 , R 2 and R 3 is at least 8; and

a vinyl aromatic, gel-type polymer which comprises repeating units represented by the formula:

wherein the benzyl chloride group is located at the meta, ortho or para position;

in a ratio of from 0.5 to 1.2 mole of tertiary amine per mole of benzyl chloride group of the polymer, within an alcohol-based solvent comprising at least: 30 weight percent methanol, 20 weight percent methylal and 10 weight percent water, to form a reaction mixture;

ii) conducting an amination reaction for a reaction time period of from 5 to 10 hours; and

iii) maintaining the reaction mixture at a temperature of from 65 to 85° C. and a pH of from 8.5 to 11.5 for at least half of the reaction time period.

Assignments (5)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 10, 2024
From: DOW GLOBAL TECHNOLOGIES LLC
To: THE DOW CHEMICAL COMPANY
Reel/Frame 069923/0030 →
CHANGE OF LEGAL ENTITY Recorded Sep 10, 2024
From: DDP SPECIALTY ELECTRONIC MATERIALS US, INC
To: DDP SPECIALTY ELECTRONIC MATERIALS US, LLC
Reel/Frame 068907/0881 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 10, 2024
From: THE DOW CHEMICAL COMPANY
To: DDP SPECIALTY ELECTRONIC MATERIALS US, INC
Reel/Frame 068922/0001 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 13, 2012
From: DOW GLOBAL TECHNOLOGIES INC
To: DOW GLOBAL TECHNOLOGIES LLC
Reel/Frame 028776/0354 →
CHANGE OF NAME Recorded Mar 21, 2011
From: DOW GLOBAL TECHNOLOGIES INC.
To: DOW GLOBAL TECHNOLOGIES LLC
Reel/Frame 025990/0796 →