Methods of manufacturing induction rotors with conductor bars having high conductivity

Inventors: Qigui Wang (Rochester Hills, MI); Mark A. Osborne (Grand Blanc, MI); Eugene C. Tuohy (Grand Blanc, MI)
Assignee: GM Global Technology Operations LLC
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,701,270
App. No.
12/691,217
Granted
Apr 22, 2014
Kind
B2
Abstract

Methods of making squirrel cage rotors of aluminum based material end rings joined with high conductive and durable material (such as copper) conductor bars for use in electric motors. The methods include forming conductor bars by casting or other metal forming methods in the slots of laminate steel stack, or positioning the preformed or premade solid conductor bars in the longitudinal slots of the stacked laminated steel, with bar ends extending out of the laminated steel stack ends, optionally coating the extended part of the conductors (bars) with a latent exoergic coating containing Al and one or more conductor bar chemical elements, positioning the laminated steel stack having conductors (bars) in a casting mold that forms the cavity of both end rings of the rotor, filling the end ring cavities with aluminum melt, and allowing the end rings to solidify under pressure. Alternatively, the conductor bars and end rings can be made separately and mechanically joined together.

Claims (24)

1. A method of making a squirrel cage rotor, the method comprising;

providing a laminated steel stack having a plurality of substantially longitudinal slots formed therein;

forming a plurality of conductor bars in the plurality of substantially longitudinal slots, each conductor bar being made of a high conductive material and having opposing first and second ends extending beyond the laminate steel stack;

coating the first ends, or the second ends, or both of the plurality of conductor bars with aluminum, aluminum alloys, a latent exoergic coating, or combinations thereof;

placing the laminated steel stack with the plurality of conductor bars in a casting mold having cavities for a pair of end rings on opposite ends of the laminated steel stack, wherein the first and second ends of the plurality of conductor bars extend into the cavities; and

filling the cavities with aluminum, aluminum alloys, aluminum composites, or combinations thereof and casting the pair of end rings;

wherein the plurality of conductor bars and the end rings are made of different materials.

2. The method of claim 1 wherein the cavities are filled using a casting method selected from high pressure die casting, low pressure die casting, sand casting, squeeze casting, centifugal casting, lost foam casting, investment casting, or combinations thereof.

3. The method of claim 1 further comprising bending the first ends, or the second ends, or both of the plurality of conductor bars before filling the cavities.

4. The method of claim 1 further comprising welding the first ends, or the second ends, or both of the plurality of conductor bars together before filling the cavities.

5. The method of claim 1 wherein the plurality of conductor bars are formed in the longitudinal slots of the laminate steel stack by a casting process or a powder metallurgy process.

6. The method of claim 1 wherein the high conductive material is copper, silver, or alloys thereof; preformed extruded pure aluminum or aluminum alloys; or copper, silver, or aluminum matrix composites containing high conductive particles, fibers, or tubes; or combinations thereof.

7. The method of claim 1 wherein the plurality of conductor bars are not perpendicular to a plane of the end ring where the plurality of conductor bars are attached.

8. A method of making a squirrel cage rotor, the method comprising;

providing a laminated steel stack having a plurality of substantially longitudinal slots formed therein;

placing a plurality of preformed conductor bars made of a high conductive material in the longitudinal slots such that first and second ends of the bars extend beyond the laminated steel stack, the first ends, the second ends, or both of the plurality of conductor bars being coated with aluminum, aluminum alloys, a latent exoergic coating, or combinations thereof;

providing a pair of end rings by placing the laminated steel stack with the plurality of conductor bars in a casting mold having cavities for a pair of end rings on opposite ends of the laminated steel stack, wherein the first and second ends of the plurality of conductor bars extend into the cavities; and filling the cavities with aluminum, aluminum alloys, aluminum composites, or combinations thereof and casting the pair of end rings;

wherein the plurality of conductor bars and the end rings are made of different materials.

9. The method of claim 8 wherein the high conductive material is copper, silver, or alloys thereof; preformed extruded pure aluminum; or copper, silver, or aluminum matrix composites containing high conductive particles, fibers, or tubes; or combinations thereof.

10. The method of claim 8 wherein the plurality of conductor bars are not perpendicular to a plane of the end ring where the plurality of conductor bars are attached.

11. The method of claim 8 further comprising bending the first ends, or the second ends, or both of the plurality of conductor bars before filling the cavities.

12. The method of claim 8 further comprising welding the first ends, or the second ends, or both of the plurality of conductor bars together before filling the cavities.

13. The method of claim 8 wherein the latent exoergic coating comprises aluminum and at least a conductor bar chemical element selected from copper, aluminum, and silver.

14. The method of claim 1 wherein the latent exoergic coating comprises aluminum and at least a conductor bar chemical element selected from copper, aluminum, and silver.

Assignments (4)
RELEASE OF SECURITY INTEREST Recorded Nov 7, 2014
From: WILMINGTON TRUST COMPANY
To: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Reel/Frame 034287/0001 →
CHANGE OF NAME Recorded Feb 10, 2011
From: GM GLOBAL TECHNOLOGY OPERATIONS, INC.
To: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Reel/Frame 025781/0333 →
SECURITY AGREEMENT Recorded Nov 8, 2010
From: GM GLOBAL TECHNOLOGY OPERATIONS, INC.
To: WILMINGTON TRUST COMPANY
Reel/Frame 025327/0156 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 21, 2010
From: WANG, QIGUI; OSBORNE, MARK A.; TUOHY, EUGENE C.
To: GM GLOBAL TECHNOLOGY OPERATIONS, INC.
Reel/Frame 023826/0293 →
Continuity (1)
Related Publication 20110175484A1 · Jul 21, 2011