IP Library Patent Application 12720692
Patent Application
App. No. 12/720,692

METHOD OF PRODUCING WHITE PIGMENT DISPERSION LIQUID AND METHOD OF PRODUCING INKJET RECORDING MEDIUM

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
12/720,692
Abstract

A method of producing a white pigment dispersion liquid includes: mixing and dispersing a white pigment, a dispersant and a medium to form a dispersion liquid in which the amount of the white pigment is 20% by mass or more relative to the total mass of the dispersion liquid; and subjecting the dispersion liquid to a depressurization treatment after the dispersing. A method of producing an inkjet recording medium includes: producing a white pigment dispersion liquid by the method of producing a white pigment dispersion liquid; preparing a coating liquid by mixing at least the white pigment dispersion liquid and a water-soluble resin; and forming an ink receiving layer by applying the coating liquid onto a support.

Claims (19)

1 . A method of producing a white pigment dispersion liquid, the method comprising:

mixing and dispersing a white pigment, a dispersant and a medium to form a dispersion liquid in which the amount of the white pigment is 20% by mass or more relative to the total mass of the dispersion liquid; and

subjecting the dispersion liquid to a depressurization treatment after the dispersing.

2 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the average primary particle diameter of the white pigment is 20 nm or less.

3 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the white pigment comprises vapor-phase process silica.

4 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the depressurization treatment is performed by reducing the pressure by 1×10 4 Pa or more.

5 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the dispersant is a cationic compound.

6 . The method of producing a white pigment dispersion liquid according to claim 5 , wherein the cationic compound comprises a diallyldimethyl cationic polymer.

7 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein each of the white pigment and the dispersant is added in more than one stage.

8 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the ratio of the dispersant relative to the white pigment is from 0.1% by mass to 30% by mass.

9 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the medium comprises an aqueous medium and the aqueous medium comprises water or a mixed medium of water and an organic solvent that is miscible with water.

10 . The method of producing a white pigment dispersion liquid according to claim 1 , wherein the duration of the depressurization treatment is 3 minutes or more.

11 . A method of producing an inkjet recording medium comprising:

producing a white pigment dispersion liquid by the method of producing a white pigment dispersion liquid according to claim 1 ;

preparing a coating liquid by mixing at least the white pigment dispersion liquid and a water-soluble resin; and

forming an ink receiving layer by applying the coating liquid onto a support.

12 . The method of producing an inkjet recording medium according to claim 11 , wherein the water-soluble resin comprises a polyvinyl alcohol resin.

13 . The method of producing an inkjet recording medium according to claim 11 , wherein the content of the water-soluble resin is from 9% by mass to 40% by mass relative to a total solid content of the coating liquid or of the ink receiving layer.

14 . The method of producing an inkjet recording medium according to claim 11 , wherein the white pigment comprises vapor-phase process silica, and the mass ratio of the vapor-phase process silica (x) to the water-soluble resin (y) [PB ratio(x/y)] is from 1.5/1 to 10/1.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 12, 2010
From: NAKANO, RYOICHI
To: FUJIFILM CORPORATION
Reel/Frame 024069/0958 →