IP Library Granted Patent US 8,664,573
Granted Patent B2
US 8,664,573 · App. 12/767,719 · Granted Mar 4, 2014

CNT-based resistive heating for deicing composite structures

Inventors: Tushar K. Shah (Columbia, MD); Harry C. Malecki (Abingdon, MD); Daniel Jacob Adcock (Columbia, MD)
Assignee: Applied NanoStructured Solutions, LLC
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,664,573
App. No.
12/767,719
Granted
Mar 4, 2014
Kind
B2
Abstract

A composite structure includes a matrix material and a carbon nanotube (CNT)-infused fiber material that includes a plurality of carbon nanotubes (CNTs) infused to a fiber material. The CNT-infused fiber material is disposed throughout a portion of the matrix material. The composite structure is adapted for application of a current through the CNT-infused fiber material to provide heating of the composite structure. A heating element includes a CNT-infused fiber material includes a plurality of CNTs infused to a fiber material. The CNT-infused fiber material is of sufficient proportions to provide heating to a structure in need thereof.

Claims (32)

1. A composite structure comprising:

a body adapted for use as a structural member of an aircraft wherein the body carries a portion of a load induced by flight of the aircraft;

a fiber substrate dispersed through a portion of the body;

a plurality of carbon nanotubes (CNTs) that have been grown in-situ on the fiber substrate so as to be aligned and oriented perpendicular to the fiber substrate, thereby forming a CNT-infused fiber material; and

a first electrode and a second electrode that are electrically coupled to the portion of the body that comprises the CNT-infused fiber material, wherein application of an electric current through the first and second electrodes and the intervening CNT-infused fiber material generates heat within the CNT-infused fiber material, thereby heating the body of the composite structure, thereby deicing or preventing ice formation on a surface of the composite structure.

2. The composite structure of claim 1 , wherein the body is adapted to form a portion of a wing of an airplane.

3. The composite structure of claim 1 , wherein the body is adapted to form a portion of a blade of a helicopter.

4. The composite structure of claim 1 , wherein the body is adapted to form a portion of a propulsor blade of an airplane.

5. The composite structure of claim 1 , further comprising a matrix material that is dispersed through the portion of the body that contains the CNT-infused fiber material.

6. The composite structure of claim 1 , wherein the fiber substrate comprises a glass.

7. The composite structure of claim 1 , wherein the fiber substrate carbon.

8. The composite structure of claim 1 , wherein the fiber substrate a ceramic.

9. The composite structure of claim 1 , wherein the plurality of CNTs have been grown as one or more of a group consisting of single-walled CNTs, double-walled CNTs, multi-walled CNTs, and mixtures thereof.

10. The composite structure of claim 1 , wherein the plurality of CNTs have been grown to be generally uniform in length and uniform in distribution.

11. The composite structure of claim 1 , wherein plurality of CNTs have been grown to have a length of about 1 micron to about 500 microns.

12. The composite structure of claim 1 , wherein the plurality of CNTs have been grown to have a length from about 1 micron to about 10 microns.

13. The composite structure of claim 1 , wherein the plurality of CNTs have been grown to have a length from about 10 microns to about 100 microns.

14. The composite structure of claim 1 , wherein the plurality of CNTs have been grown to have a length from about 100 microns to about 500 microns.

15. The composite structure of claim 1 , wherein the plurality of CNTs have been grown to have a uniformity of distribution that is characterized by a density up to about 15,000 nanotubes per square micrometer.

16. The composite structure of claim 1 , wherein the fiber substrate is selected from a filament, a tow, a yarn, a tape, a unidirectional tape, a fiber-braid, a woven fabric, a non-woven fiber mat, a fiber ply, and a 3D woven structure.

17. The composite structure of claim 1 , wherein the CNT-infused fiber material is disposed near a surface of the body.

18. The composite structure of claim 1 , wherein the CNT-infused fiber material is disposed throughout the entire.

19. The composite structure of claim 5 , wherein the matrix material comprises one or more of a group consisting of an epoxy, a phenolic resin, a cement, a glass, a thermoplastic, and a thermoset.

20. The composite structure of claim 1 , wherein the electric current is created by application of a direct current (DC) voltage from between about 1 to about 24 volts DC.

21. The composite structure of claim 1 , wherein the electric current is created by application of an alternating current (AC) voltage between about 60 and about 480 volts AC.

22. A method, comprising the steps of:

growing a plurality of carbon nanotubes (CNTs) in-situ on a fiber substrate such that the CNTs are aligned and oriented perpendicular to the fiber substrate, thereby forming a CNT-infused fiber material;

forming a composite structure of an aircraft, wherein the composite structure is adapted to carry a portion of a load induced by flight of the aircraft, the composite structure having a body having a portion that comprises the CNT-infused fiber material;

electrically coupling a first electrode and a second electrode to the portion of the body that comprises the CNT-infused fiber material, wherein application of an electric current through the first and second electrodes and the intervening CNT-infused fiber generates heat within the CNT-infused fiber material, thereby heating the body of the composite structure, thereby deicing or preventing ice formation on a surface of the composite structure.

23. The method of claim 22 , wherein the step of applying an electric current comprises applying a direct current (DC) voltage that is between about 1 and about 24 volts DC.

24. The method of claim 22 , wherein the step of applying an electric current comprises applying a alternating current (AC) voltage that is between about 60 and about 480 volts AC.

25. The composite structure of claim 19 , further comprising a plurality of loose CNTs disposed within the matrix material.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 7, 2011
From: LOCKHEED MARTIN CORPORATION
To: APPLIED NANOSTRUCTURED SOLUTIONS, LLC
Reel/Frame 025913/0473 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 24, 2010
From: SHAH, TUSHAR K.; MALECKI, HARRY C.; ADCOCK, DANIEL JACOB
To: LOCKHEED MARTIN CORPORATION
Reel/Frame 024591/0184 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 6, 2010
From: LOCKHEED MARTIN CORPORATION
To: APPLIED NANOSTRUCTURED SOLUTIONS, LLC
Reel/Frame 024349/0133 →
Continuity (2)
Provisional Application 61173027 · Apr 27, 2009
Related Publication 20110024409A1 · Feb 3, 2011