US 8,450,600 · App. 12/801,849 · Granted May 28, 2013

Photovoltaic device with scratch-resistant coating

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,450,600
App. No.
12/801,849
Granted
May 28, 2013
Kind
B2
Abstract

A method of making an anti-reflection coating using a sol-gel process, for use in a photovoltaic device or the like. The method may include the following steps in certain example embodiments: forming a polymeric component of silica by mixing silane(s) with one or more of a first solvent, a catalyst, and water; forming a silica sol gel by mixing the polymeric component with a colloidal silica, and optionally a second solvent; forming a metal oxide sol by mixing silane(s) with a metal oxide, a second catalyst, and a third solvent; forming a combined sol by mixing the metal oxide sol with the silica sol; casting the mixture by spin coating or the like to form a silica and metal oxide containing layer on a substrate; and curing and/or heat treating the layer. This layer may make up all or only part of an anti-reflection coating which may be used in a photovoltaic device or the like.

Claims (23)

1. A photovoltaic device comprising:

a photovoltaic film, and at least a glass substrate on a light incident side of the photovoltaic film;

an anti-reflection coating provided on the glass substrate;

wherein the anti-reflection coating comprises at least a layer provided directly on and contacting the glass substrate, wherein the layer comprises porous silica and a metal oxide and wherein the layer comprising porous silica and the metal oxide comprises less than 5% of the metal oxide by weight, and wherein the layer comprising porous silica and the metal oxide comprises anorthite.

2. The photovoltaic device of claim 1 , wherein the glass substrate comprises a soda-lime-silica glass including the following ingredients: SiO 2 , 67-75% by weight;

Na 2 O, 10-20% by weight; CaO, 5-15% by weight; MgO, 0-7% by weight; Al 2 O 3 , 0-5% by weight; K 2 O, 0-5% by weight; Li 2 O, 0-1 5% by weight; and BaO, 0-1%, by weight.

3. The photovoltaic device of claim 1 , wherein the metal oxide further comprises one or more of: 3Al 2 O 3 :2SiO 2 , Al 2 O 3 : SiO 2 , Mg Al 2 O 4 , ZrO 2 , and Al 2 O 3 .

4. The photovoltaic device of claim 1 , wherein the anti-reflection coating further comprises a layer comprising an oxide of silicon located over and contacting the layer comprising porous silica and the metal oxide.

5. The photovoltaic device of claim 1 , wherein the layer comprising porous silica and the metal oxide comprises a critical scratch load of from about 40 to 70 mN.

6. The photovoltaic device of claim 1 , wherein the anti-reflection coating comprises a critical scratch load of from about 40to 70mN.

7. The photovoltaic device of claim 1 , wherein the layer comprising porous silica and the metal oxide comprises a critical scratch load of from about 70 to 80 mN.

8. The photovoltaic device of claim 1 , wherein the anti-reflection coating comprises a critical scratch load of from about 70 to 80 mN.

9. The photovoltaic device of claim 1 , wherein the layer comprising porous silica and the metal oxide comprises a critical scratch load of from about 80 to 120 mN.

10. The photovoltaic device of claim 1 , wherein the anti-reflection coating comprises a critical scratch load of from about 80 to 120 mN.

11. A photovoltaic device comprising:

a photovoltaic film, and at least a glass substrate on a light incident side of the photovoltaic film;

an anti-reflection coating provided on the glass substrate;

wherein the anti-reflection coating comprises a first layer comprising porous silica and a metal oxide provided directly on and contacting the glass substrate, wherein the first layer comprises anorthite; and

a second layer comprising an oxide of silica provided over and contacting the first layer, wherein the anti-reflection coating comprises a critical scratch load of from about 40 to 120 mN.

12. The photovoltaic device of claim 11 , wherein the first layer further comprises mullite, silimanite, and/or spinels.

13. The photovoltaic device of claim 11 , wherein the first layer comprises less than about 5% metal oxide by weight.

14. The photovoltaic device of claim 1 , wherein the layer comprising porous silica and the metal oxide comprises about 2% metal oxide by weight.

15. The photovoltaic device of claim 13 , wherein the first layer comprises about 2% metal oxide by weight.