IP Library Granted Patent US 8,535,482
Granted Patent B2
US 8,535,482 · App. 12/851,121 · Granted Sep 17, 2013

Dry fluff pulp sheet additive

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,535,482
App. No.
12/851,121
Granted
Sep 17, 2013
Kind
B2
Abstract

A process is provided for making a fluff pulp sheet, comprising forming a web comprising fluff pulp fibers; and applying at least one debonder surfactant to the web, to make the fluff pulp sheet. A fluff pulp sheet is also provided, comprising a web comprising fluff pulp fibers; at least one debonder surfactant; and a fiberization energy of <145 kJ/kg. Products and uses of the fluff pulp sheet are also provided.

Claims (19)

1. A process for making a fluff pulp sheet, comprising:

forming, on a table of a papermaking machine, a web comprising fluff pulp fibers; and

spraying at least one debonder surfactant onto the web, wherein said spraying is carried out on the table and prior to a dryer section, to make the fluff pulp sheet;

wherein the debonder surfactant is one or more selected from the group consisting of linear or branched monoalkyl amine, linear or branched dialkyl amine, linear or branched tertiary alkyl amine, linear or branched quaternary alkyl amine, fatty acid amide, fatty acid amide quaternary ammonium salt, dialkyl dimethyl quaternary ammonium salt, dialkylimidazolinium quaternary ammonium salt, dialkyl ester quaternary ammonium salt, triethanolamine-ditallow fatty acid, dialkyl amide of fatty acid, dialkyl amide of fatty acid, compound having CAS Registry No. 68155-01-1, compound having CAS Registry No. 26316-40-5, and a combination thereof.

2. The process of claim 1 , wherein the forming comprises one or more of contacting a fluff pulp mixture comprising fluff pulp fibers and water with the table, removing at least a portion of water from a fluff pulp mixture comprising fluff pulp fibers and water with a suction box under the table, heating a fluff pulp mixture comprising fluff pulp fibers and water, heating the debonder surfactant, or a combination thereof.

3. The process of claim 1 , wherein the spraying is carried out using one or more formation showers over the table.

4. The process of claim 1 , wherein the web has a basis weight of 100 to 1100 gsm.

5. The process of claim 1 , wherein the web further comprises water and optionally one or more debonder surfactant, pH adjusting agent, whitener, colorant, pigment, optical brightening agent, wetting agent, binder, bleaching agent, trivalent cationic metal, alum, other additive, or a combination thereof.

6. The process of claim 1 , wherein the web comprises a solids content of >1% by weight.

7. The process of claim 1 , wherein the debonder surfactant is neat, in combination with one or more second debonder surfactant, in solution, or combination thereof.

8. The process of claim 1 , wherein the debonder surfactant is in the form of a composition further comprising water and optionally one or more pH adjusting agent, whitener, colorant, pigment, optical brightening agent, wetting agent, binder, bleaching agent, trivalent cationic metal, alum, other additive, or a combination thereof.

9. The process of claim 1 , further comprising fiberizing or shredding the fluff pulp sheet.

10. The process of claim 9 , wherein the fiberizing or shredding are carried out in a hammermill.

11. The process of claim 1 , further comprising incorporating the fluff pulp sheet into one or more of an adsorbent product, paper product, personal care product, medical product, insulating product, construction product, structural material, cement, food product, veterinary product, packaging product, diaper, tampon, sanitary napkin, gauze, bandage, fire retardant or a combination thereof.

12. The process of claim 1 , wherein the debonder surfactant is applied as a solution, dispersion, or emulsion at a concentration of 1 to 50% by weight solids content of debonder surfactant to the weight of the solution, dispersion, or emulsion.

13. The process of claim 1 , further comprising spraying a second debonder surfactant onto the fluff pulp sheet.

14. The process of claim 1 , further comprising, after the spraying, drying the web to a moisture content of between 0 and 70%.

15. The process of claim 1 , wherein the debonder surfactant is present in an amount of 1 to 20 lbs per ton of fluff pulp fibers.

16. The process of claim 1 , wherein the debonder surfactant is present in an amount of 1 to 4 lbs per ton of fluff pulp fibers.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 14, 2025
From: INTERNATIONAL PAPER COMPANY
To: GCF US HOLDINGS LLC
Reel/Frame 073563/0717 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 28, 2010
From: JIANG, JIANER
To: INTERNATIONAL PAPER COMPANY
Reel/Frame 025052/0358 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 28, 2010
From: SEALEY, JAMES E.
To: INTERNATIONAL PAPER COMPANY
Reel/Frame 025052/0382 →