Crumb rubber modified asphalt with improved stability

Assignee: Innophos, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,211,960
App. No.
12/903,786
Granted
Jul 3, 2012
Kind
B2
Abstract

The present invention relates to a method for producing a crumb rubber modified asphalt comprising the steps of: a) heating a pre-selected quantity of asphalt to a temperature of between about 325° F. to 550° F.; b) adding crumb rubber and a mineral acid to the heated asphalt with stirring; and c) blowing air through the asphalt, crumb rubber and mineral acid mixture.

Claims (9)

1. A method for producing a crumb rubber modified asphalt comprising the steps of:

a) heating a pre-selected quantity of asphalt to a temperature of between about 325° F. to 550° F.;

b) adding crumb rubber and a mineral acid to the heated asphalt with stirring; and

c) blowing air through the asphalt, crumb rubber and mineral acid mixture.

2. The method of claim 1 , wherein the crumb rubber is ground tire rubber and is added to achieve a crumb rubber level of between about 0.5% to 25% by weight of the weight of the asphalt, crumb rubber and mineral acid mixture.

3. The method of claim 2 , wherein the crumb rubber has a mesh size between about 10 mesh and about 200 mesh.

4. The method of claim 3 , wherein the mineral acid is polyphosphoric acid and is added to achieve an acid level of between about 0.05% to about 5% by weight of the weight of the asphalt, crumb rubber and mineral acid mixture.

5. The method of claim 4 , further comprising the step of blowing air through the asphalt, crumb rubber and mineral acid mixture while stirring.

6. The method of claim 5 , wherein the asphalt, crumb rubber and mineral acid mixture is stirred for a period of between about 1 hour and about 24 hours.

Assignments (2)
PATENT SECURITY AGREEMENT (ABL) Recorded Feb 10, 2020
From: INNOPHOS, INC.; INNOPHOS, LLC
To: ROYAL BANK OF CANADA, AS COLLATERAL AGENT
Reel/Frame 051858/0131 →
PATENT SECURITY AGREEMENT (TL) Recorded Feb 10, 2020
From: INNOPHOS, INC.; INNOPHOS, LLC
To: ROYAL BANK OF CANADA, AS COLLATERAL AGENT
Reel/Frame 051858/0161 →
Continuity (2)
Provisional Application 61251163 · Oct 13, 2009
Related Publication 20110160356A1 · Jun 30, 2011