Barrier film composite, display apparatus including the barrier film composite, and method of manufacturing display apparatus including the barrier film composite

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,412,970
App. No.
12/981,353
Granted
Aug 9, 2016
Kind
B2
Abstract

A barrier film composite includes a heat-shrinkable layer having a conformable surface conforming to a surface shape of an object in contact with the heat-shrinkable layer, and a flat surface disposed opposite to the conformable surface; and a barrier layer having a smaller thickness than the heat-shrinkable layer and disposed flat on the flat surface of the heat-shrinkable layer.

Claims (9)

1. A method of manufacturing a display apparatus, the method comprising:

forming a light-emitting device on a substrate;

independently from the formation of the light-emitting device, providing a barrier film composite comprising a heat-shrinkable layer having a predetermined thickness and a barrier layer that is disposed on a surface of the heat-shrinkable layer, the heat-shrinkable layer having a conformable surface conforming to a shape of a surface of an object when the surface of the object is in direct physical contact with the heat-shrinkable layer and a flat surface disposed opposite to and spaced apart from the conformable surface, the barrier layer extending throughout an entirety of the flat surface disposed opposite to and spaced apart from the conformable surface; and

aligning the barrier film composite to the substrate in such a manner that the heat-shrinkable layer contacts the light-emitting device and simultaneously applying pressure and heat to the heat-shrinkable layer to remove an air gap between the light-emitting device and the heat-shrinkable layer,

wherein a minimum thickness of the heat-shrinkable layer is larger than a thickness of the barrier layer, and the barrier layer is disposed farther from the light-emitting device than the heat-shrinkable layer.

2. The method of claim 1 , wherein in the step of applying heat to the heat-shrinkable layer, the heat-shrinkable layer shrinks so that a surface of the heat-shrinkable layer physically contacting the light-emitting device conforms to a surface shape of the light-emitting device and removes an air gap between the light-emitting device and the heat-shrinkable layer.

3. The method of claim 1 , wherein in the step of aligning the barrier film composite to the light-emitting device, applying a predetermined pressure to the barrier film composite.

4. The method of claim 1 , wherein the barrier film composite comprises a plurality of alternating layers of the heat-shrinkable layer and the barrier layer.

5. The method of claim 1 , wherein in the forming of the light-emitting device, the light-emitting device comprises an organic light-emitting device.

Assignments (2)
MERGER Recorded Sep 21, 2012
From: SAMSUNG MOBILE DISPLAY CO., LTD.
To: SAMSUNG DISPLAY CO., LTD.
Reel/Frame 029241/0599 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 13, 2011
From: HAN, DONG-WON; VISSER, ROBERT JAN; MORO, LORENZA
To: SAMSUNG MOBILE DISPLAY CO., LTD., A CORPORATION CHARTERED IN AND EXISTING UNDER THE LAWS OF THE REPUBLIC OF KOREA
Reel/Frame 026478/0089 →