IP Library Granted Patent US 8,456,803
Granted Patent B2
US 8,456,803 · App. 13/003,043 · Granted Jun 4, 2013

Method for production of electrolyte capacitors

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,456,803
App. No.
13/003,043
Granted
Jun 4, 2013
Kind
B2
Abstract

The invention relates to a process for producing electrolytic capacitors with low equivalent series resistance, to electrolytic capacitors produced by this process and to the use of such electrolytic capacitors.

Claims (26)

1. A process for producing an electrolytic capacitor, at least comprising, that

a) onto a porous body, at least comprising

a porous electrode body of an electrode material and a dielectric which covers the surface of this electrode material,

is applied a dispersion A)

which comprises at least particles B) of an electrically conductive polymer and a dispersant D),

b) and a solid electrolyte which partly or fully covers the dielectric surface is formed by at least partly removing the dispersant D),

characterized in that the pH of the dispersion A) measured at 25° C. is greater than or equal to 1.8 and less than or equal to 3.9.

2. The process according to claim 1 , characterized in that particles B) of dispersion A) in the dry state have a specific electrical conductivity of greater than 100 S/cm.

3. The process according to claim 1 , characterized in that the particles B) of the conductive polymer in dispersion A) have a mean diameter of 1-100 nm.

4. The process according to claim 1 , characterized in that the dispersion A) has a content of metals of less than 5000 mg/kg.

5. The process according to claim 1 , characterized in that the particles B) in dispersion A) comprise at least one polythiophene with repeat units of the general formula (I) or of the general formula (II) or of the general formula (X) or repeat units of the formulae (I) and (II) or repeat units of the formulae (I) and (X) or repeat units of the formulae (II) and (X) or repeat units of the formulae (I), (II) and (X)

in which

A is an optionally substituted C 1 -C 5 -alkylene radical,

R is independently H, a linear or branched, optionally substituted C 1 -C 18 -alkyl radical, an optionally substituted C 5 -C 12 -cycloalkyl radical, an optionally substituted C 6 -C 14 -aryl radical, an optionally substituted C 7 -C 18 -aralkyl radical, an optionally substituted C 1 -C 4 -hydroxyalkyl radical or a hydroxyl radical,

x is an integer of 0 to 8 and,

in the case that a plurality of R radicals is bonded to A, they may be the same or different.

6. The process according to claim 1 , characterized in that the conductive polymer in dispersion A) is an optionally substituted poly(3,4-ethylenedioxythiophene).

7. The process according to claim 1 , characterized in that the particles B) additionally comprise at least one polymeric anion.

8. The process according to claim 7 , characterized in that the polymeric anion is an anion of a polymeric carboxylic or sulphonic acid.

9. The process according to claim 1 , characterized in that the dispersion A) comprises, as the dispersant D), organic solvents, water or mixtures of organic solvents and water.

10. The process according to claim 1 , characterized in that dispersion A) additionally comprises crosslinkers, surface-active substances, further additives, or combinations thereof.

11. The process according to claim 1 , characterized in that the electrode material of the electrode body is a valve metal or a compound with properties comparable to a valve metal.

12. An electrolytic capacitor produced by a process according to claim 1 .

13. A method comprising using the electrolytic capacitors according to claim 12 in electronic circuits.

14. An electronic circuit comprising an electrolytic capacitor according to claim 13 .

15. A dispersion comprising at least particles comprising an electrically conductive polythiophene, which is optionally substituted, and a dispersant, characterized in that the pH of the dispersion measured at 25° C. is greater than or equal to 1.8 and less than or equal to 3.9, and in that the particles comprising a polythiophene, in the dry state, possess a specific electrical conductivity greater than 100 S/cm.

Assignments (4)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 7, 2024
From: HERAEUS DEUTSCHLAND GMBH & CO. KG
To: HERAEUS EPURIO GMBH
Reel/Frame 067330/0850 →
CHANGE OF NAME Recorded Nov 6, 2015
From: HERAEUS PRECIOUS METALS GMBH & CO. KG
To: HERAEUS DEUTSCHLAND GMBH & CO. KG
Reel/Frame 037056/0430 →
MERGER Recorded Feb 21, 2012
From: HERAEUS CLEVIOS GMBH
To: HERAEUS PRECIOUS METALS GMBH & CO. KG
Reel/Frame 027734/0357 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 7, 2011
From: MERKER, UDO; WUSSOW, KLAUS
To: H.C. STARCK CLEVIOS GMBH
Reel/Frame 025754/0454 →