Method of making demineralized bone particles
View Patent ↗Demineralized bone particles are obtained by demineralizing whole bone and thereafter subdividing the demineralized bone to provide the demineralized bone particles.
1. A method of making demineralized bone particles which comprises demineralizing whole bone and thereafter subdividing the demineralized bone into demineralized bone particles wherein at least about 80 weight percent of the particles have a median length to width ratio of from about 2 to 200, wherein the yield of demineralized bone particles is greater than that obtained by subdividing the whole bone into mineralized bone particles and thereafter demineralizing the mineralized bone particles to provide demineralized bone particles, wherein subdividing of the demineralized bone is carried out by applying pressure to the demineralized bone using a mechanical press, wherein the pressure is applied from 1,000 to about 40,000 psi.
2. The method of claim 1 , wherein the whole bone is demineralized to contain less than about 10% by weight residual calcium.
3. The method of claim 1 , wherein the whole bone is demineralized to contain less than about 5% by weight residual calcium.
4. The method of claim 1 , wherein the whole bone is demineralized to contain less than about 1% by weight residual calcium.
5. The method of claim 1 , wherein the bone is subjected to being pressed while being unconstrained.
6. The method of claim 1 , wherein the bone is subjected to being pressed while being constrained.