Treated electrolytic manganese dioxide and method for its production
View Patent ↗A method for preparing treated electrolytic manganese dioxide and a battery including the treated electrolytic manganese dioxide as an electrode are provided. The method for treating the electrolytic manganese dioxide includes suspending milled electrolytic manganese dioxide in an aqueous solution heated to a temperature between ambient and boiling, and adjusting an acidity of the aqueous solution to a pH of less than 3.3. The method further includes agitating the suspended milled electrolytic manganese dioxide in the aqueous solution for a predetermined amount of time to dissolve metal-containing particulates in the milled electrolytic manganese dioxide.
1. A method for preparing treated electrolytic manganese dioxide, the method comprising:
suspending milled non-neutralized electrolytic manganese dioxide in an aqueous solution heated to a temperature above 29° C. up to boiling;
controlling an acidity of the aqueous solution to maintain a pH of less than 3.3, but at least 1.7; and
agitating the suspended non-neutralized milled electrolytic manganese dioxide in the aqueous solution for a predetermined amount of time selected to dissolve metal-containing particulates in the milled electrolytic manganese dioxide.
2. The method of claim 1 , wherein the suspending comprises heating the aqueous solution to a temperature ranging from 30° C. to 70° C.
3. The method of claim 1 , wherein the predetermined time comprises a time ranging from 30 minutes to 3 hours.
4. The method of claim 1 , wherein the predetermined time comprises a time of less than 2 hours.
5. The method of claim 1 , wherein the adjusting comprises adding sulfuric acid to adjust the acidity of the aqueous solution.
6. The method of claim 1 , wherein the aqueous solution is not saturated with dissolved copper ions or iron ions.
7. The method of claim 1 , wherein the predetermined amount of time is an amount of time between 30 minutes to 120 minutes.